Ageing of plasma-treated poly(tetrafluoroethylene) surfaces

被引:91
作者
Nakamatsu, J [1 ]
Delgado-Aparicio, LF [1 ]
Da Silva, R [1 ]
Soberón, F [1 ]
机构
[1] Pontificia Univ Catolica Peru, Dept Sci, Lima 100, Peru
关键词
plasma treatment; surface modification; ageing; poly(tetrafluoraethylene); contact angle;
D O I
10.1163/156856199X00983
中图分类号
TQ [化学工业];
学科分类号
0817 ;
摘要
Highly hydrophobic poly(tetrafluoroethylene) (PTFE) surfaces were modified with an air glow discharge plasma to improve their wettability. However, the hydrophilic character obtained diminishes with time, due to molecular movement in the polymer. We have determined that the ageing process is strongly affected by the environment and temperature in which the surfaces are stored. A hydrophobic environment and high temperatures promote faster recovery of the original properties of PTFE than low temperatures. Nonetheless, a hydrophilic environment, even at high temperatures, prevents the surface from losing the polar character obtained from the plasma treatment, stopping the ageing process. Moreover, this process is reversible since the character of the treated surface changes when the environment changes (i.e. from water to air). The hydrophilicity of the surfaces was evaluated by contact angle measurements of a droplet of water.
引用
收藏
页码:753 / 761
页数:9
相关论文
共 18 条
[1]   DEPTH SENSITIVITY OF WETTING - MONOLAYERS OF OMEGA-MERCAPTO ETHERS ON GOLD [J].
BAIN, CD ;
WHITESIDES, GM .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1988, 110 (17) :5897-5898
[2]   INVESTIGATION OF THE AGING OF PLASMA OXIDIZED PEEK [J].
BRENNAN, WJ ;
FEAST, WJ ;
MUNRO, HS ;
WALKER, SA .
POLYMER, 1991, 32 (08) :1527-1530
[3]  
Chan JTH, 1996, CONTROL COMPUT, V24, P1
[4]   SURFACE-SELECTIVE INTRODUCTION OF SPECIFIC FUNCTIONALITIES ONTO POLY(TETRAFLUOROETHYLENE) [J].
COSTELLO, CA ;
MCCARTHY, TJ .
MACROMOLECULES, 1987, 20 (11) :2819-2828
[5]  
Denes F, 1997, TRENDS POLYM SCI, V5, P23
[6]   PLASMA MODIFICATION OF POLYMER SURFACES FOR ADHESION IMPROVEMENT [J].
EGITTO, FD ;
MATIENZO, LJ .
IBM JOURNAL OF RESEARCH AND DEVELOPMENT, 1994, 38 (04) :423-439
[7]   Hydrophobic recovery of repeatedly plasma-treated silicone rubber .2. A comparison of the hydrophobic recovery in air, water, or liquid nitrogen [J].
Everaert, EP ;
VanderMei, HC ;
Busscher, HJ .
JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 1996, 10 (04) :351-359
[8]   HYDROPHOBIC RECOVERY OF REPEATEDLY PLASMA-TREATED SILICONE-RUBBER .1. STORAGE IN AIR [J].
EVERAERT, EP ;
VANDERMEI, HC ;
DEVRIES, J ;
BUSSCHER, HJ .
JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 1995, 9 (09) :1263-1278
[9]   PLASMA SURFACE MODIFICATION OF POLYETHYLENE - SHORT-TERM VS LONG-TERM PLASMA TREATMENT [J].
FOERCH, R ;
KILL, G ;
WALZAK, MJ .
JOURNAL OF ADHESION SCIENCE AND TECHNOLOGY, 1993, 7 (10) :1077-1089
[10]   Surface modification and functionalization of polytetrafluoroethylene films [J].
Kang, ET ;
Tan, KL ;
Kato, K ;
Uyama, Y ;
Ikada, Y .
MACROMOLECULES, 1996, 29 (21) :6872-6879