Electron-lattice coupling parameters and oscillator strengths of cerium-doped lutetium oxyorthosilicate

被引:56
作者
Cooke, DW [1 ]
Bennett, BL
McClellan, KJ
Roper, JM
Whittaker, MT
Portis, AM
机构
[1] Univ Calif Los Alamos Natl Lab, Div Mat Sci & Technol, Los Alamos, NM 87545 USA
[2] Univ Calif Berkeley, Dept Phys, Berkeley, CA 94720 USA
来源
PHYSICAL REVIEW B | 2000年 / 61卷 / 18期
关键词
D O I
10.1103/PhysRevB.61.11973
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Optical absorption of single-crystal, cerium-doped lutetium oxyorthosilicate has been carefully measured in the temperature interval 10-300 K. Prominent Gaussian absorption peaks occur at 3.432+/-0.002 eV (peak a), 3.502+/-0.002 eV (peak b), 4.236+/-0.0002 eV (peak c), and 4.746+/-0.0002 eV (peak d), in excellent agreement with previously reported excitation spectra. The second moments are well described by the usual linear model, yielding the Huang-Rhys parameter (S) and vibrational quantum energies for the individual peaks. All absorption bands are characterized by S>5 indicating strong coupling between the Ce3+ ion and lattice. Temperature dependence of the band centroids exhibits contrasting behavior that is dominated by higher-order coupling terms in the linear harmonic oscillator model or by crystal-field effects. Oscillator strengths of the 4f-->5d transitions are calculated from Smakula's formula and knowledge of the Ce3+ distribution between the two crystallographically inequivalent sites. Values for peaks b, c, and d range from approximately 0.003 to 0.004, and peak a spans magnitude approximately 0.012 to 0.018. From the known correlation between average Ce3+-ion-ligand distance and oscillator strength, we tentatively conclude that peak a is correlated with the seven-oxygen-coordinated site, and peaks b, c, and d are associated with the six-oxygen-coordinated site. These results support the previously proposed two-activation-center model and identify the centers as the two crystallographically inequivalent substitutional sites.
引用
收藏
页码:11973 / 11978
页数:6
相关论文
共 24 条
[1]  
BLASSE G, 1994, LUMINESCENT MAT, P46
[2]  
BLASSE G, 1991, ADV NONRADIATIVE PRO, P291
[3]   CZOCHRALSKI GROWTH OF RARE-EARTH ORTHOSILICATES (LN2SIO5) [J].
BRANDLE, CD ;
VALENTINO, AJ ;
BERKSTRESSER, GW .
JOURNAL OF CRYSTAL GROWTH, 1986, 79 (1-3) :308-315
[4]  
DEXTER DL, 1958, SOLID STATE PHYS, V6, P353
[5]  
DIBARTOLO B, 1968, OPTICAL INTERACTIONS, P420
[6]   SCINTILLATION AND THERMOLUMINESCENCE PROPERTIES OF LU2SIO5CE FAST SCINTILLATION CRYSTALS [J].
DORENBOS, P ;
VANEIJK, CWE ;
BOS, AJJ ;
MELCHER, CL .
JOURNAL OF LUMINESCENCE, 1994, 60-1 :979-982
[7]   AFTERGLOW AND THERMOLUMINESCENCE PROPERTIES OF LU2SIO5-CE SCINTILLATION CRYSTALS [J].
DORENBOS, P ;
VANEIJK, CWE ;
BOS, AJJ ;
MELCHER, CL .
JOURNAL OF PHYSICS-CONDENSED MATTER, 1994, 6 (22) :4167-4180
[8]  
HAMILTON TDS, 1978, LUMINESCENCE SPECTRO, P151
[9]  
Huang K, 1950, P ROY SOC LOND A MAT, V204, P404
[10]  
HUGHES AE, 1972, POINT DEFECTS SOLIDS, V1, P412