Characterization of Li-V-O nanorod phases and their effect on electrochemical properties of Li1+xV3O8 cathode materials synthesized by hydrothermal reaction and subsequent heat treatment

被引:19
作者
Kim, Kyungho [1 ]
Park, Su Han [1 ]
Kwon, Tae Hyung [1 ]
Park, Ji Eun [1 ]
Ahn, Hyungkeun [2 ]
Lee, Man-Jong [1 ]
机构
[1] Konkuk Univ, Dept Adv Technol Fus, Seoul 143701, South Korea
[2] Konkuk Univ, Dept Elect Engn, Seoul 143701, South Korea
基金
新加坡国家研究基金会;
关键词
LiV3O8; cathode; Li0.3V2O5; Li-V-O nanorods; Electrochemical properties; EIS; RECHARGEABLE LITHIUM BATTERY; LIV3O8; NANORODS; PERFORMANCE; CAPACITY; IMPROVEMENT; IMPEDANCE;
D O I
10.1016/j.electacta.2012.11.106
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
Lithium vanadium oxide (Li1+xV3O8, x=0.2) cathode materials were synthesized via a simple hydrothermal reaction followed by heat treatment at elevated temperatures, and the electrochemical performance of as-synthesized LiV3O8 as a cathode material for lithium ion batteries was investigated using galvanostatic discharge-charge cycling and electrochemical impedance spectroscopy. It reveals that different thermal treatment histories resulted in drastic changes in sizes/morphologies and electrochemical properties. The samples that were heat treated at 300 degrees C contained many nanorod-like particles, particularly at the surface of agglomerated LiV3O8 particles. Such nanorod-shaped Li-V-O compounds exhibit two different crystal structures: either a defective LiV3O8 or a Li0.3V2O5 structure. In addition, the nanorod-shaped Li-V-O compounds in the galvanostatically cycled samples could not be observed using high-resolution scanning electron microscopy (HRSEM) because of their structural instability, which can be attributed to the deterioration of their electrochemical properties during cycling. In contrast, the samples treated at 400 and 500 degrees C exhibited a bi-modal particle distribution and estimated sheet-like morphologies with no impurities, respectively. They also indicated excellent electrochemical properties. (C) 2012 Elsevier Ltd. All rights reserved.
引用
收藏
页码:708 / 716
页数:9
相关论文
共 42 条
[1]   Atomic structure and electrochemical potential of Li1+xV3O8 [J].
Benedek, R ;
Thackeray, MM ;
Yang, LH .
PHYSICAL REVIEW B, 1999, 60 (09) :6335-6342
[2]   Rechargeable lithium batteries based on Li1+xV3O8 thin films [J].
Bonino, F ;
Panero, S ;
Pasquali, M ;
Pistoia, G .
JOURNAL OF POWER SOURCES, 1995, 56 (02) :193-196
[3]   Phase formation and electrochemical properties of cryochemically processed Li1+xV3O8 materials [J].
Brylev, Oleg A. ;
Shlyakhtin, Oleg A. ;
Egorov, Alexander V. ;
Tretyakov, Yuri D. .
JOURNAL OF POWER SOURCES, 2007, 164 (02) :868-873
[4]   Probing Li-Ni Cation Disorder in Li1-xNi1+x-yAlyO2 Cathode Materials by Neutron Diffraction [J].
Cai, Lu ;
Liu, Zengcai ;
An, Ke ;
Liang, Chengdu .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2012, 159 (07) :A924-A928
[5]   Using radial basis functions to approximate battery differential capacity and differential voltage [J].
Christophersen, Jon P. ;
Shaw, Steven R. .
JOURNAL OF POWER SOURCES, 2010, 195 (04) :1225-1234
[6]   STRUCTURAL CHARACTERIZATION OF LI1+XV3O8 INSERTION ELECTRODES BY SINGLE-CRYSTAL X-RAY-DIFFRACTION [J].
DEPICCIOTTO, LA ;
ADENDORFF, KT ;
LILES, DC ;
THACKERAY, MM .
SOLID STATE IONICS, 1993, 62 (3-4) :297-307
[7]   Formation of Li1+nV3O8/β-Li1/3V2O5/C nanocomposites by carboreduction and the resulting improvement in Li capacity retention [J].
Dubarry, M ;
Gaubicher, J ;
Moreau, P ;
Guyomard, D .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2006, 153 (02) :A295-A300
[8]   APPLICATION OF AC TECHNIQUES TO THE STUDY OF LITHIUM DIFFUSION IN TUNGSTEN TRIOXIDE THIN-FILMS [J].
HO, C ;
RAISTRICK, ID ;
HUGGINS, RA .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1980, 127 (02) :343-350
[9]   The origin of capacity fading upon lithium cycling in Li1.1V3O8 [J].
Jouanneau, S ;
La Salle, AL ;
Verbaere, A ;
Guyomard, D .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2005, 152 (08) :A1660-A1667
[10]   Influence of the morphology on the Li insertion properties of Li1.1V3O8 [J].
Jouanneau, S ;
La Salle, AL ;
Verbaere, A ;
Deschamps, M ;
Lascaud, S ;
Guyomard, D .
JOURNAL OF MATERIALS CHEMISTRY, 2003, 13 (04) :921-927