Corrosion and polarization behavior of sensitized high-nitrogen stainless steels

被引:11
作者
Covino, BS
Cramer, SD
Russell, JH
Simmons, JW
机构
[1] U.S. Department of Energy, Albany Research Center, Albany, OR 97321, 1450 Queen Ave., SW
关键词
austenitic stainless steel; degree of sensitization; dichromium nitride; energy dispersive spectroscopy; inductively coupled plasma spectroscopy; nitrogen; potentiodynamic polarization testing; scanning electron microscopy; scanning transmission electron microscopy; sensitization; stainless steels; x-ray diffraction;
D O I
10.5006/1.3290284
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Corrosion of a sensitized high-nitrogen stainless steel (SS, nominally Fe-19% Cr-5% Ni-5% Mn-3% Mo-0.024% C-0.69% N) was studied by examining potentiodynamic polarization curves. Corrosion behavior was compared to previously reported sensitization values. The SS was heat treated at temperatures of 600 degrees C to 1,000 degrees C for times up to 1,000 h. Potentiodynamic polarization curves were generated in deaerated 1 N sulfuric acid (H2SO4) + 0.01 M potassium thiocyanate (KSCN) at 30 degrees C at a scan rate of 100 mV/min. Corrosion currents measured at the corrosion potential did not change in the same manner with increasing aging time as values for the degree of sensitization (DOS). This was believed to be caused by greater sensitivity to chromium depletion during potentiodynamic polarization testing compared to sensitization measured by electrochemical potentiokinetic reactivation (EPR) testing (i.e., the minimum chromium level in the depletion zone required to cause sensitization, approximate to 14 wt%, was lower than that required to degrade corrosion behavior as measured by potentiodynamic polarization testing). Polarization curves exhibited two oxidation peaks in the active region and two in the passive region. All were functions of aging time and temperature. Solution analyses as a function of applied potential and x-ray diffraction (XRD) analyses were used to help identify the matrix components that might be responsible for those peaks.
引用
收藏
页码:525 / 536
页数:12
相关论文
共 27 条
[1]  
*ASTM, 1992, ASTM BOOK STANDARDS, P449
[2]   PROPERTIES OF NITROGEN-CONTAINING STAINLESS ALLOY DESIGNED FOR HIGH-RESISTANCE TO PITTING [J].
BANDY, R ;
VANROOYEN, D .
CORROSION, 1985, 41 (04) :228-233
[3]  
Berns H., 1988, P 1 INT C HIGH NITR, P288
[4]  
BRUEMMER SM, 1988, THESIS OREGON GRADUA
[5]   POLARIZATION AND RESISTIVITY MEASUREMENTS OF POST-CRYSTALLIZATION CHANGES IN AMORPHOUS FE-B-SI ALLOYS [J].
CHATTORAJ, I ;
BHATTAMISHRA, AK ;
MITRA, A .
CORROSION, 1993, 49 (09) :707-713
[6]  
Chernova G.P., 1980, ZASHCH MET, V16, P3
[7]  
CHIGIRINSKAYA LA, 1984, PROT MET+, V20, P320
[8]   THE SENSITIZATION AND STRESS-CORROSION CRACKING OF NITROGEN-CONTAINING STAINLESS-STEELS [J].
DUTTA, RS ;
DE, PK ;
GADIYAR, HS .
CORROSION SCIENCE, 1993, 34 (01) :51-60
[9]   INTERPRETATION OF PASSIVE CURRENT MAXIMA DURING POLARIZATION OF STAINLESS STEELS [J].
FRANCE, WD ;
GREENE, ND .
CORROSION, 1968, 24 (12) :403-&
[10]  
GOYKHENBERG YN, 1991, PHYS MET METALLOGR, V72, P179