Profluorescent nitroxides: Sensors and stabilizers of radical-mediated oxidative damage

被引:32
作者
Blinco, James P. [1 ]
Keddie, Daniel J. [1 ]
Wade, Tim [1 ]
Barker, Philip J. [2 ]
George, Graeme A. [1 ]
Bottle, Steven E. [1 ]
机构
[1] Queensland Univ Technol, ARC Ctr Excellence Free Rad Chem & Biotechnol, Brisbane, Qld Q4001, Australia
[2] BlueScope Steel Res, Port Kembla, NSW 2505, Australia
基金
澳大利亚研究理事会;
关键词
profluorescent nitroxide; fluorescence; polypropylene; crosslinked polyester; thermal oxidation; photo-oxidation;
D O I
10.1016/j.polymdegradstab.2008.05.028
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
In this study, three profluorescent nitroxides 1,1,3,3-tetramethyldibenzo[e,g]isoindolin-2-yloxyl (TMDBIO), 1,1,3,3-tetramethyl-2,3-dihydro-2-azaphenalene-2-yloxyl (TMAO) and 5-[2-(4-methoxycarbonyl-phenyl)-ethenyl]1,1,3,3-tetramethylisoindoline-2-yloxyl (MeCSTMIO) were tested as probes for radical-mediated damage in polypropylene arising from both UV and thermally initiated sources. These nitroxides possess a very low fluorescence quantum yield due to quenching by the nitroxide group; however, when the free-radical moiety is removed by reaction with alkyl radicals (to give an alkoxyamine), strong fluorescence is observed. The results obtained from this profluorescent nitroxide trapping technique compare favourably with other methods of monitoring degradation, provided the appropriate probe is chosen for the conditions of oxidation. signalling an indication of damage well before other techniques show any response. The technique was also applied to the monitoring of crosslinked polyester coating resins. Differentiation in the oxidative stability of the resins was evident after as little as 200 min where other monitoring techniques require up to 300 h of accelerated degradation. This highlights the sensitivity of this method as well as demonstrating the scope of this technique to assess polymer stability. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1613 / 1618
页数:6
相关论文
共 11 条
[1]   The first example of an azaphenalene profluoreseent nitroxide [J].
Blinco, James P. ;
McMurtrie, John C. ;
Bottle, Steven E. .
EUROPEAN JOURNAL OF ORGANIC CHEMISTRY, 2007, 2007 (28) :4638-4641
[2]   CHEMILUMINESCENCE IMAGING OF THE OXIDATION OF POLYPROPYLENE [J].
CELINA, M ;
GEORGE, GA ;
LACEY, DJ ;
BILLINGHAM, NC .
POLYMER DEGRADATION AND STABILITY, 1995, 47 (02) :311-317
[3]   Photochemical stability and photo stabilizing efficiency of anthracene/hindered amine stabilizers in polymer matrices [J].
Danko, M ;
Chmela, T ;
Hrdlovic, P .
POLYMER DEGRADATION AND STABILITY, 2003, 79 (02) :333-343
[4]   A study of the effects of postcure treatments on polyester-melamine coating matrices [J].
Gamage, NJW ;
Hill, DJT ;
Pomery, PJ ;
Lukey, CA .
POLYMER ENGINEERING AND SCIENCE, 2006, 46 (04) :532-539
[5]   Catalyst residue effects on the heterogeneous oxidation of polypropylene [J].
Goss, Ben G.S. ;
Nakatani, H. ;
George, Graeme A. ;
Terano, M. .
Polymer Degradation and Stability, 2003, 82 (01) :119-126
[6]   Spectral characteristics and photochemical stability of fluorescence probes based on 1,8-naphthaleneimide in solution and in polymer matrix [J].
Hrdlovic, P ;
Chmela, S ;
Danko, M .
JOURNAL OF PHOTOCHEMISTRY AND PHOTOBIOLOGY A-CHEMISTRY, 1998, 112 (2-3) :197-203
[7]   Synthesis of profluorescent isoindoline nitroxides via palladium-catalysed Heck alkenylation [J].
Keddie, DJ ;
Johnson, TE ;
Arnold, DP ;
Bottle, SE .
ORGANIC & BIOMOLECULAR CHEMISTRY, 2005, 3 (14) :2593-2598
[8]   UV photolysis of melamine formaldehyde crosslinkers [J].
Lukey, CA ;
Hill, DJT ;
Pomery, PJ .
POLYMER DEGRADATION AND STABILITY, 2002, 78 (03) :485-490
[9]   The use of chemiluminescence analysis to measure hydroperoxide levels in photo-oxidised polyester/melamine surface coatings [J].
Lukey, CA .
PROGRESS IN ORGANIC COATINGS, 2001, 41 (1-3) :129-134
[10]   The application of a novel profluorescent nitroxide to monitor thermo-oxidative degradation of polypropylene [J].
Micallef, AS ;
Blinco, JP ;
George, GA ;
Reid, DA ;
Rizzardo, E ;
Thang, SH ;
Bottle, SE .
POLYMER DEGRADATION AND STABILITY, 2005, 89 (03) :427-435