Frictional behavior of self-adaptive nanostructural Mo-Se-C coatings in different sliding conditions

被引:32
作者
Gustavsson, E. [1 ]
Jacobson, S. [1 ]
Cavaleiro, A. [2 ]
Polcar, T. [3 ]
机构
[1] Uppsala Univ, Dept Engn Sci, Angstrom Tribomat Grp, S-75121 Uppsala, Sweden
[2] Univ Coimbra, Dept Mech Engn, SEG CEMUC, P-3030788 Coimbra, Portugal
[3] Czech Tech Univ, Fac Elect Engn, Dept Control Engn, CR-16635 Prague 6, Czech Republic
基金
加拿大自然科学与工程研究理事会; 瑞典研究理事会;
关键词
Solid lubricants; MoSe2; Friction; Tribolayer; Self-adaptive structure; TRIBOLOGICAL PROPERTIES; WEAR; OXIDATION; SUPERLUBRICITY; MECHANISMS; CHEMISTRY; SPECTRA; CARBON; FILMS;
D O I
10.1016/j.wear.2013.03.032
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
Sliding properties of Mo-Se-C coatings with two different carbon content deposited by magnetron sputtering were investigated in different sliding environments (argon, nitrogen, dry and humid air). Both coatings had a structure that was identified as randomly oriented structures of MoSe2 embedded into amorphous carbon matrix. The worn surfaces, i.e. the wear tracks and the wear scars of the balls, were analyzed by optical microscopy, Raman spectroscopy and scanning electron microscopy. The material transferred to the ball steel surfaces was almost exclusively MoSe2, whereas the wear tracks on the coatings were more complex, with areas rich in MoSe2 and areas similar to that of as-deposited coatings. The friction was lowest in argon (0.012 at a load of 10 N) and highest in humid air, but still remarkably low; as best 0.05 at 10 N load; however, the exceptionally low wear rate was almost identical. Thus, we focused our detailed analysis on these two examples to understand the mechanisms responsible for the difference between the friction coefficients. SEM, EDX, XPS, Raman and TEM with EELS and EDX were applied to investigate the composition and structure of localized spots of interest on the tested surfaces. In both cases, we observed well-ordered MoSe2 tribofilms with negligible amount of oxides. Carbon was not present in the sliding interfaces, although large amount of carbon was found outside the contacts on both surfaces. Based on our investigations, we suggest the increase in friction of Mg-Se-C in humid air is primarily due to the increase in shear strength of the MoSe2 structure by the presence of water molecules in the sliding interface. (C) 2013 Elsevier B.V. All rights reserved.
引用
收藏
页码:286 / 296
页数:11
相关论文
共 43 条
[1]   Friction of diamond-like carbon films in different atmospheres [J].
Andersson, J ;
Erck, RA ;
Erdemir, A .
WEAR, 2003, 254 (11) :1070-1075
[3]  
Brainard W.A., 1969, The Thermal Stability and Friction of the Disulfides, Diselenides, and Ditellurides of Molybdenum and Tungsten in Vacuum
[4]   Super-low friction of MoS2 coatings in various environments [J].
Donnet, C ;
Martin, JM ;
LeMogne, T ;
Belin, M .
TRIBOLOGY INTERNATIONAL, 1996, 29 (02) :123-128
[5]  
Dukstiene N, 2010, MATER SCI-POLAND, V28, P93
[6]   Synthesis and properties of W-Se-C coatings deposited by PVD in reactive and non-reactive processes [J].
Evaristo, Manuel ;
Polcar, Tomas ;
Cavaleiro, Albano .
VACUUM, 2009, 83 (10) :1262-1265
[7]   Interpretation of Raman spectra of disordered and amorphous carbon [J].
Ferrari, AC ;
Robertson, J .
PHYSICAL REVIEW B, 2000, 61 (20) :14095-14107
[8]   A comparison of oxidation and oxygen substitution in MoS2 solid film lubricants [J].
Fleischauer, PD ;
Lince, JR .
TRIBOLOGY INTERNATIONAL, 1999, 32 (11) :627-636
[9]   Pulsed laser deposition of composite Mo-Se-Ni-C coatings using standard and shadow mask configuration [J].
Fominski, V. Yu. ;
Grigoriev, S. N. ;
Gnedovets, A. G. ;
Romanov, R. I. .
SURFACE & COATINGS TECHNOLOGY, 2012, 206 (24) :5046-5054
[10]   Structure and mechanical properties of W-Se-C/diamond-like carbon and W-Se/diamond-like carbon bi-layer coatings prepared by pulsed laser deposition [J].
Fominski, V. Yu. ;
Grigoriev, S. N. ;
Celis, J. P. ;
Romanov, R. I. ;
Oshurko, V. B. .
THIN SOLID FILMS, 2012, 520 (21) :6476-6483