Functionally graded bioactive coatings: Reproducibility and stability of the coating under cell culture conditions

被引:33
作者
Foppiano, S
Marshall, SJ
Saiz, E
Tomsia, AP
Marshall, GW
机构
[1] Univ Calif San Francisco, Div Biomat & Bioengn, San Francisco, CA 94143 USA
[2] Univ Calif Berkeley, Lawrence Berkeley Lab, Div Mat Sci, Berkeley, CA 94720 USA
关键词
bioactive glass; osteoblasts; coating; simulated body fluid;
D O I
10.1016/j.actbio.2005.12.003
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
This work sought to provide a basic protocol for treatment of functionally graded bioactive glass coatings (FGC) that reliably adhere to titanium alloy (Ti6Al4V) prior to in vivo evaluation. The effect of the fabrication process on glass structure and reproducibility of the coating's properties, and the effect of cell culture conditions on the integrity of the coating were assessed. The structure of FGCs was compared to that of the as cast glass used as a top coating. X-ray diffraction (XRD) showed that the fabrication process resulted in 5.9 +/- 3.0 vol.% crystallization, while glass as cast was amorphous. Glass as cast and coatings behaved similarly in simulated body fluid (SBF): an amorphous layer rich in phosphate formed, and it crystallized, over 4 weeks, into apatite-like mineral (Fourier transform infrared spectroscopy (FTIR), XRD, scanning electron microscopy (SEM)). Reproducibility of the fabrication process was tested from three batches of coatings by measuring thickness and crystallinity. MC3T3-E1.4 mouse pre-osteoblast cells were cultured and induced to mineralize on FGCs, either as made or pre-conditioned in SBF. The sub-surface glass silica network in FGCs was compromised by cell culture conditions. A crystalline phosphate was formed during pre-conditioning (XRD, FTIR, and SEM). SBF-pre-conditioning stabilized the coatings. Thus incubation in SBF is recommended to produce a stable coating. (c) 2006 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:133 / 142
页数:10
相关论文
共 53 条
[1]  
[Anonymous], 1994, STUDIES INORGANIC CH
[2]  
ASHBY MF, 1980, ENG MAT INTRO THEIR, P129
[3]  
BLOEBAUM RD, 1993, J ARTHROPLASTY, V8, P203, DOI 10.1016/S0883-5403(09)80014-4
[4]   BIOCOMPATIBILITY OF NITINOL ALLOY AS AN IMPLANT MATERIAL [J].
CASTLEMAN, LS ;
MOTZKIN, SM ;
ALICANDRI, FP ;
BONAWIT, VL ;
JOHNSON, AA .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1976, 10 (05) :695-731
[5]  
Chang YL, 1999, J ORAL MAXIL SURG, V57, P1096
[6]  
CHANG YL, 1999, J ORAL MAXILLOFAC SU, V75, P1108
[7]   EFFECT OF BIOACTIVE GLASS TEMPLATES ON OSTEOBLAST PROLIFERATION AND IN-VITRO SYNTHESIS OF BONE-LIKE TISSUE [J].
DUCHEYNE, P ;
ELGHANNAM, A ;
SHAPIRO, I .
JOURNAL OF CELLULAR BIOCHEMISTRY, 1994, 56 (02) :162-167
[8]   THE EFFECT OF CALCIUM-PHOSPHATE CERAMIC COMPOSITION AND STRUCTURE ON INVITRO BEHAVIOR .1. DISSOLUTION [J].
DUCHEYNE, P ;
RADIN, S ;
KING, L .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1993, 27 (01) :25-34
[9]   CALCIUM-PHOSPHATE CERAMIC COATINGS ON POROUS TITANIUM - EFFECT OF STRUCTURE AND COMPOSITION ON ELECTROPHORETIC DEPOSITION, VACUUM SINTERING AND INVITRO DISSOLUTION [J].
DUCHEYNE, P ;
RADIN, S ;
HEUGHEBAERT, M ;
HEUGHEBAERT, JC .
BIOMATERIALS, 1990, 11 (04) :244-254
[10]   Formation of surface reaction products on bioactive glass and their effects on the expression of the osteoblastic phenotype and the deposition of mineralized extracellular matrix [J].
ElGhannam, A ;
Ducheyne, P ;
Shapiro, IM .
BIOMATERIALS, 1997, 18 (04) :295-303