Cavitation erosion mechanism of NiTi coatings made by laser plasma hybrid spraying

被引:130
作者
Hiraga, H
Inoue, T
Shimura, H
Matsunawa, A
机构
[1] Appl Laser Engn Res Inst, Nagaoka, Niigata 9402135, Japan
[2] Agcy Ind Sci & Technol, Mech Engn Lab, Tsukuba, Ibaraki, Japan
[3] Osaka Univ, Joining & Welding Res Inst, Ibaraki, Osaka, Japan
关键词
plasma spraying; CO2; laser; surface treatment; intermetallic compound; work hardening; super elasticity;
D O I
10.1016/S0043-1648(99)00133-7
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
NiTi intermetallic compound is known to be a high cavitation erosion-resistant material. The erosion behaviors of NiTi intermetallic compound coatings made by laser plasma hybrid spraying (LPHS) were studied. The erosion resistance of the NiTi coatings depended strongly on the chemical composition of the coatings and the laser irradiation condition, because the NiTi phase and the microstructure of the coatings were varied by those conditions. The best erosion-resistant coatings were obtained with the conditions of nickel composition richer than that of equiatomic NiTi and irradiated laser power density greater than 6 x 10(8) W/m(2). The cavitation erosion resistance of the coating was about 380-fold that of a titanium alloy substrate. High erosion resistance of these coatings was obtained due to a combination of two factors, namely, super elasticity due to austenite-phase NiTi and high work hardenability due to excess soluble Ni. (C) 1999 Elsevier Science S.A. All rights reserved.
引用
收藏
页码:272 / 278
页数:7
相关论文
共 10 条
[1]  
[Anonymous], 1962, ASM T
[2]   INFLUENCE OF WORK-HARDENING AND HEAT-TREATMENT ON THE SUBSTRUCTURE AND DEFORMATION-BEHAVIOR OF TINI SHAPE-MEMORY ALLOYS [J].
FILIP, P ;
MAZANEC, K .
SCRIPTA METALLURGICA ET MATERIALIA, 1995, 32 (09) :1375-1380
[3]  
GUO XX, 1986, ADV THERMAL SPRAYING, P37
[4]  
HEYMANN FJ, 1970, ASTM STP, V474, P212, DOI DOI 10.1520/STP474-EB
[5]  
HIRAGA H, 1996, P IC 96 DETR US, P200
[6]   SHAPE MEMORY EFFECT BY DIFFUSIONAL TRANSFORMATION IN TI-52-PERCENT-NI ALLOY [J].
KAINUMA, R ;
MATSUMOTO, M .
SCRIPTA METALLURGICA, 1988, 22 (04) :475-478
[7]  
NAKAO E, 1995, PREPRINT JAPAN SOC M, V72, P206
[8]  
RICHMAN RH, 1995, WEAR, V181, P80, DOI 10.1016/0043-1648(95)90011-X
[9]   CAVITATION EROSION OF 2 NITI ALLOYS [J].
RICHMAN, RH ;
RAO, AS ;
HODGSON, DE .
WEAR, 1992, 157 (02) :401-407
[10]  
ZHOU KS, 1988, THERMAL SPRAY ADV CO, P167