Carbon-fibre-reinforced (YMAS) glass-ceramic matrix composites .1. Preparation, structure and fracture strength

被引:9
作者
Bianchi, V
Goursat, P
Sinkler, W
Monthioux, M
Menessier, E
机构
[1] CNRS,UPRESA 6015,CEMES,F-31055 TOULOUSE,FRANCE
[2] CERAM & COMPOSITES,F-65460 BAZET,FRANCE
关键词
OXIDATION BEHAVIOR; CRACKING; FIBERS; MICROTEXTURE; MECHANICS;
D O I
10.1016/S0955-2219(97)00004-6
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
Unidirectional continuous carbon-fibre-reinforced glass-ceramic matrix composites are fabricated for dry sliding applications. The microstructure of the matrix has been characterized by X-ray diffraction and the microtexture and structure of the fibres (pitch-based and PAN-based) have been studied by transmission electronic microscopy. The different fracture behaviours of the composites are described (three-point bend rest and fracture surface observation by scanning electronic microscopy). Due to the thermal expansion mismatch between the fibres and the matrix, a network of microcracks appears in the composites on cooling after hot-pressing. The relationship between the microcrack spacing and the fracture behaviour suggests modifications of the fibre-matrix bond. (C) 1997 Elsevier Science Limited.
引用
收藏
页码:1485 / 1500
页数:16
相关论文
共 28 条
  • [1] Aveston J., 1971, Conference Proceedings, National Physical Laboratory (IPC Science and Technology Press Ltd), P15
  • [2] Aveston J., 1971, PROPERTIES FIBRE COM, P63
  • [3] BIANCHI V, 1994, ADV STRUCTURAL FIBER, V7, P695
  • [4] BIANCHI V, 1995, THESIS LIMOGES U FRA
  • [5] BIANCHI V, UNPUB J EUR CERAM SO
  • [6] MATRIX FRACTURE IN FIBER-REINFORCED CERAMICS
    BUDIANSKY, B
    HUTCHINSON, JW
    EVANS, AG
    [J]. JOURNAL OF THE MECHANICS AND PHYSICS OF SOLIDS, 1986, 34 (02) : 167 - 189
  • [7] DESPRES JF, 1992, ETUDE INTERFACES COM
  • [8] DESPRES JF, 1993, THESIS PAU PAYS ADOU
  • [9] STRUCTURE AND REACTIVITY OF CARBONS - FROM CARBON-BLACK TO CARBON COMPOSITES
    DONNET, JB
    [J]. CARBON, 1982, 20 (04) : 267 - 282
  • [10] MICROTEXTURE AND STRUCTURE OF SOME HIGH-TENSILE STRENGTH, PAN-BASE CARBON-FIBERS
    GUIGON, M
    OBERLIN, A
    DESARMOT, G
    [J]. FIBRE SCIENCE & TECHNOLOGY, 1984, 20 (01): : 55 - 72