Bi4V2O11 and related compounds as positive electrode materials for lithium rechargeable batteries

被引:21
作者
deDompablo, MEAY [1 ]
GarciaAlvarado, F [1 ]
Moran, E [1 ]
机构
[1] UNIV COMPLUTENSE MADRID,FAC CIENCIAS QUIM,DEPT QUIM INORGAN,E-28040 MADRID,SPAIN
关键词
lithium intercalation; electrode materials; lithium batteries; irreversibility;
D O I
10.1016/S0167-2738(96)83029-3
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
In the search for new intercalation electrode materials, several phases related to the compound Bi4V2O11 have been tested as positive electrodes in room temperature electrochemical lithium cells. Bi4V2O11, Bi3.6Pb0.4V2O11-y and Bi4V1.8Cu0.22O11-y are structurally similar compounds differing only from a microstructural point of view. Electrochemical lithium intercalation is not affected by such structural and compositional differences, since the performance of all these phases is equivalent. The surprising amount of 8 lithium ions per vanadium atom inserted in Bi4V2O11 during the first discharge at an average potential of 1.7 V implies a theoretical specific energy of 655 Wh/Kg. In spite of this promising value, the irreversibility found after the first discharge slightly reduces the possibilities of these materials as positive electrodes in room temperature rechargeable lithium batteries. Even so, the energy density is high enough to consider the materials for future improvements.
引用
收藏
页码:273 / 278
页数:6
相关论文
共 12 条
[1]   COMPRESSED CU2+ IONS IN A BI4V2O11 OXIDE MATRIX .1. EPR AND UV-VISIBLE STUDY [J].
ABOUKAIS, A ;
DELMAIRE, F ;
RIGOLE, M ;
HUBAUT, R ;
MAIRESSE, G .
CHEMISTRY OF MATERIALS, 1993, 5 (12) :1819-1822
[2]   THE BIMEVOX SERIES - A NEW FAMILY OF HIGH PERFORMANCES OXIDE ION CONDUCTORS [J].
ABRAHAM, F ;
BOIVIN, JC ;
MAIRESSE, G ;
NOWOGROCKI, G .
SOLID STATE IONICS, 1990, 40-1 (pt 2) :934-937
[3]   PHASE-TRANSITIONS AND IONIC-CONDUCTIVITY IN BI4V2O11 AN OXIDE WITH A LAYERED STRUCTURE [J].
ABRAHAM, F ;
DEBREUILLEGRESSE, MF ;
MAIRESSE, G ;
NOWOGROCKI, G .
SOLID STATE IONICS, 1988, 28 :529-532
[4]  
AURIVILLIUS B, 1949, ARK KEMI, V0001
[5]  
BESENHARD JO, 1978, Z NATURFORSCH B, V33, P279
[6]  
DEDOMPABLO EAY, IN PRESS
[7]   CRYSTAL-STRUCTURE OF LOW-TEMPERATURE FORM OF BISMUTH VANADIUM-OXIDE DETERMINED BY RIETVELD REFINEMENT OF X-RAY AND NEUTRON-DIFFRACTION DATA (ALPHA-BI4V2O11) [J].
JOUBERT, O ;
JOUANNEAUX, A ;
GANNE, M .
MATERIALS RESEARCH BULLETIN, 1994, 29 (02) :175-184
[8]  
Julien C., 1994, Solid State Batteries: Materials Design and Optimization
[9]   PHASE-DIAGRAMS AND STOICHIOMETRIES OF THE SOLID ELECTROLYTES, BI4V2O11-M, M=CO, CU, ZN, CA, SR [J].
LEE, CK ;
LIM, GS ;
WEST, AR .
JOURNAL OF MATERIALS CHEMISTRY, 1994, 4 (09) :1441-1444
[10]   EFFECT OF ALIOVALENT-CATION SUBSTITUTION ON THE OXYGEN-ION CONDUCTIVITY OF BI4V2O11 [J].
SHARMA, V ;
SHUKLA, AK ;
GOPALAKRISHNAN, J .
SOLID STATE IONICS, 1992, 58 (3-4) :359-362