摘要
Ceramics of the two compositions of KTa(1-x)Nb(x)O(3) (KTN) with x = 0.3 and 0.4 have been densified thanks to the addition of LiF. Densities been determined as a function of sintering temperature, time and amount of LiF. Dielectric investigations have shown that the composition corresponding to x = 0.4 is more densified than x = 0.3. The two compositions x = 0.3 and x = 0.4 exhibit a paraelectric-ferroelectric phase transition at about 310 and 360 K respectively. The phase transition is more diffuse for x = 0.3. Oxygen is partially substituted for fluorine in the crystalline network.
引用
收藏
页码:41 / 51
页数:11
相关论文
共 13 条
[1]  
Debely P. E., 1979, CERAMIC B, V56, P606
[2]   DIFFUSE PHASE-TRANSITION IN CO DOPED BARIUM-TITANATE [J].
GODEFROY, G ;
CHATRY, P ;
BENGUIGUI, L .
FERROELECTRICS, 1981, 34 (04) :169-174
[3]  
Hevall J. A., 1968, SOLID STATE CHEM, P37
[4]   EXPERIMENTAL STUDIES ON QUANTUM FERROELECTRICS [J].
HOCHLI, UT .
FERROELECTRICS, 1981, 35 (1-4) :17-30
[5]  
Kingery, 1967, INTRO CERAMICS
[6]  
LU ZG, 1992, J PHYS CHEM SOLIDS, V53, P1, DOI 10.1016/0022-3697(92)90004-W
[7]  
Lu Zhigao, 1992, Journal of the European Ceramic Society, V9, P381, DOI 10.1016/0955-2219(92)90097-W
[8]   EFFECTS OF GRAIN-SIZE AND POROSITY ON ELECTRICAL AND OPTICAL PROPERTIES OF PLZT CERAMICS [J].
OKAZAKI, K ;
NAGATA, K .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1973, 56 (02) :82-86
[9]  
RAVEZ J, 1991, EUR J SOL STATE INOR, V28, P1107
[10]   CRYSTAL-GROWTH OF KTA1-XNBXO3 (0-LESS-THAN-X-LESS-THAN-OR-EQUAL-TO-0.04) SOLID-SOLUTIONS BY A SLOW-COOLING METHOD [J].
RYTZ, D ;
SCHEEL, HJ .
JOURNAL OF CRYSTAL GROWTH, 1982, 59 (03) :468-484