Injectable and self-curing composites of acrylic/bioactive glass and drug systems.: A histomorphometric analysis of the behaviour in rabbits

被引:14
作者
Corchón, MAG
Salvado, M
de la Torre, BJ
Collía, F
de Pedro, JA
Vázquez, B
Román, JS
机构
[1] CSIC, Inst Ciencia & Tecnol Polimeros, E-28006 Madrid, Spain
[2] Univ Salamanca, Fac Med, Salamanca 37007, Spain
关键词
PMMA; bioactive bone cement; bioactive glass; fosfosal; in vivo experiments; histomorphometric analysis;
D O I
10.1016/j.biomaterials.2005.10.015
中图分类号
R318 [生物医学工程];
学科分类号
0831 [生物医学工程];
摘要
Injectable self-curing systems based on PMMA, phosphate-free bioactive glasses and the drug fosfosal, a phosphate derivative of salicylic acid with analgesic and moderate anti-inflammatory properties, have been tested in vivo to evaluate their biocompatibility. The model consisted of the injection of dough of cement into a defect created in the femur of rabbits, and the cure of the cement in situ after implantation. The biological response was studied in the short and long, terms by macroscopic, radiological and histopathological examination, and quantitatively by histornorphometric and statistical analysis considering the most representative variables at the bone-cement interface: cement, bone marrow, newly formed bone and connective tissue. All bioactive formulations presented resorption of the cement at the end of the experiment in contrast to the control of PMMA, due to the presence of resorbable components. The presence or absence of the phosphate group added by the drug fosfosal influenced mainly on the new bone formation process. The cement formulated with bioactive glasses and in absence of fosfosal produced the maximum amount of neoformed bone at 2 weeks, and then it resorbed at 4 weeks to give a higher amount of neoformed bone at the end of the experiment, compared with the formulation containing only fosfosal. The presence of fosfosal and bioactive glass together affected the ossification process strongly. The osseous tissue was produced more gradually but it continuously increased giving rise to a more stable bone at the end of the experiment. (C) 2005 Elsevier Ltd. All rights reserved.
引用
收藏
页码:1778 / 1787
页数:10
相关论文
共 24 条
[1]
BARON R, 1983, BONE HISTOMORPHOMETR, P37
[2]
Biocompatibility and other properties of acrylic bone cements prepared with antiseptic activators [J].
de la Torre, B ;
Fernández, M ;
Vázquez, B ;
Collía, F ;
de Pedro, JA ;
López-Bravo, A ;
San Román, J .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH PART B-APPLIED BIOMATERIALS, 2003, 66B (02) :502-513
[3]
DELATORRE B, UNPUB J MAT SCI MAT
[4]
Mixture of ε-caprolactone-lactide copolymer and tricalcium phosphate:: a histological and immunohistochemical study of tissue reactions [J].
Ekholm, M ;
Hietanen, J ;
Lindqvist, C ;
Rautavuori, J ;
Santavirta, S ;
Salo, A ;
Seppälä, J ;
Suuronen, R .
JOURNAL OF MATERIALS SCIENCE-MATERIALS IN MEDICINE, 1999, 10 (02) :69-74
[5]
OBSERVATIONS UPON THE INTERFACE BETWEEN BONE AND POLYMETHYLMETHACRYLATE CEMENT [J].
FREEMAN, MAR ;
BRADLEY, GW ;
REVELL, PA .
JOURNAL OF BONE AND JOINT SURGERY-BRITISH VOLUME, 1982, 64 (04) :489-493
[6]
A comparative study between in vivo bone ingrowth and in vitro apatite formation on Na2O-CaO-SiO2 glasses [J].
Fujibayashi, S ;
Neo, M ;
Kim, HM ;
Kokubo, T ;
Nakamura, T .
BIOMATERIALS, 2003, 24 (08) :1349-1356
[7]
Polymethylmethacrylate composites: Disturbed bone formation at the surface of bioactive glass and hydroxyapatite [J].
Heikkila, JT ;
Aho, AJ ;
Kangasniemi, I ;
YliUrpo, A .
BIOMATERIALS, 1996, 17 (18) :1755-1760
[8]
Hench L.L., 1971, Journal of Biomedical Materials Research Symposium, V36, P117, DOI DOI 10.1002/JBM.820050611
[9]
Izquierdo-Barba I, 1999, J BIOMED MATER RES, V47, P243, DOI 10.1002/(SICI)1097-4636(199911)47:2<243::AID-JBM15>3.0.CO
[10]
2-S