A synthetic polymer matrix for the delayed or pulsatile release of water-soluble peptides

被引:24
作者
Schachter, DM [1 ]
Kohn, J [1 ]
机构
[1] Rutgers State Univ, Dept Chem, Piscataway, NJ 08854 USA
关键词
delayed release; pulsatile release; peptide-polymer interactions; tyrosine-derived polymers; polyarylate; Integrilin (TM); peptide release; poly(DTH adipate); poly(lactic-co-glycolic acid);
D O I
10.1016/S0168-3659(01)00487-4
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The design of a polymeric peptide release system with a controlled delay time and a burst-free pre-release phase is described. In general, the system consists of a blend of a tyrosine-derived polyarylate and a fast-degrading copolymer of lactic and glycolic acid (PLGA). Due to the peptide-like structure of the polyarylate backbone, peptide-polymer interactions prevented the release of peptide from neat polyarylate films. The addition of PLGA acts as a 'delayed' excipient: as PLGA degrades, it generates acidic degradation products that cause a drop in the internal pH of the polyarylate matrix. This drop in pH weakens the peptide-polymer interactions and causes the release of peptide to commence. The initial molecular weight of PLGA can be used to control the length of time before degradation occurs. Consequently, this parameter can also be used to control the duration of the delay period prior to peptide release. As a specific model system, blends of poly(DTH adipate) with three different copolymers of lactic and glycolic acid were prepared and used for the delayed release of Integrilin(TM), a synthetic water-soluble heptapeptide (clinically used in antithrombic injections) that acts as a highly potent glycoprotein IIb/IIIa antagonist. Blends composed of a 1:1 weight ratio of poly(DTH adipate) and PLGA and containing Integrilin(TM) (15%, w/w) were prepared. In vitro release studies were conducted in phosphate buffered solution at 37degreesC and the release of Integrilin(TM) was followed by HPLC, As the initial molecular weight of PLGA varied from 12 000 to 62 000, the duration of the delay period prior to release increased from 5 to 28 days. (C) 2002 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:143 / 153
页数:11
相关论文
共 23 条
[1]  
Brocchini S, 1998, J BIOMED MATER RES, V42, P66, DOI 10.1002/(SICI)1097-4636(199810)42:1<66::AID-JBM9>3.0.CO
[2]  
2-M
[3]   A combinatorial approach for polymer design [J].
Brocchini, S ;
James, K ;
Tangpasuthadol, V ;
Kohn, J .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1997, 119 (19) :4553-4554
[4]   Development of a single-shot subunit vaccine for HIV-1 .4. Optimizing microencapsulation and pulsatile release of MN rgp120 from biodegradable microspheres [J].
Cleland, JL ;
Lim, A ;
Barron, L ;
Duenas, ET ;
Powell, MF .
JOURNAL OF CONTROLLED RELEASE, 1997, 47 (02) :135-150
[5]   Hydrogen bonding and electrostatic interaction contributions to the interaction of a cationic drug with polyaspartic acid [J].
Ehtezazi, T ;
Govender, T ;
Stolnik, S .
PHARMACEUTICAL RESEARCH, 2000, 17 (07) :871-878
[6]   DYNAMIC MEMBRANES FOR PROTEIN-TRANSPORT - CHEMICAL AND ELECTRICAL CONTROL [J].
GRIMSHAW, PE ;
GRODZINSKY, AJ ;
YARMUSH, ML ;
YARMUSH, DM .
CHEMICAL ENGINEERING SCIENCE, 1989, 44 (04) :827-840
[7]   DEVELOPMENT OF ENZYMATICALLY DEGRADABLE PROTECTIVE COATINGS FOR USE IN TRIGGERED DRUG DELIVERY SYSTEMS - DERIVATIZED STARCH HYDROGELS [J].
HELLER, J ;
PANGBURN, SH ;
ROSKOS, KV .
BIOMATERIALS, 1990, 11 (05) :345-350
[8]  
HELLER J, 1990, PULSED SELF REGULATE, P94
[9]  
HOLLAND S J, 1986, Journal of Controlled Release, V4, P155, DOI 10.1016/0168-3659(86)90001-5
[10]   Hydrogen bonds in poly(ester amide)s and their model compounds [J].
Kaczmarczyk, B ;
Sek, D .
POLYMER, 1995, 36 (26) :5019-5025