Stress corrosion cracking behavior of X70 pipe steel in an acidic soil environment

被引:230
作者
Liu, Z. Y. [1 ]
Li, X. G. [1 ]
Du, C. W. [1 ]
Zhai, G. L. [1 ]
Cheng, Y. F. [2 ]
机构
[1] Univ Sci & Technol Beijing, Sch Mat Sci & Engn, Beijing 100083, Peoples R China
[2] Univ Calgary, Dept Mech & Mfg Engn, Calgary, AB T2N 1N4, Canada
关键词
Steel; Polarization; SEM; Stress corrosion;
D O I
10.1016/j.corsci.2008.05.011
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Stress corrosion cracking (SCC) behavior of X70 pipe steel was investigated in an extracted acidic soil solution by slow strain rate test (SSRT), potentiodynamic polarization curve measurements and surface analysis technique. The SCC process and mechanism of X70 steel in the acidic soil solution is mixed-controlled by both anodic dissolution and the hydrogen involvement. With the different applied potentials, the dominance of SCC process changes. At a relatively less negative potential, the steel SCC is based primarily on the anodic dissolution mechanism. When the applied potential is shifted negatively, hydrogen is involved in the cracking process, resulting in a transgranular cracking mode. With the further negative shift of applied potential, the SCC of the steel follows completely a hydrogen-based mechanism, with a river-bed shaped brittle feature of the fracture surface. Heat treatment alters the microstructure of the steel, resulting in a change of SCC susceptibility. In particular, the quenched steel with a bainite microstructure has a high susceptibility to SCC in the acidic soil, while the as-received steel with a ferrite matrix have a low SCC susceptibility. (C) 2008 Elsevier Ltd. All rights reserved.
引用
收藏
页码:2251 / 2257
页数:7
相关论文
共 26 条
[1]   Cyclic crack growth rates of X-60 pipeline steel in a neutral dilute solution [J].
Ahmed, TM ;
Lambert, SB ;
Sutherby, R ;
Plumtree, A .
CORROSION, 1997, 53 (07) :581-590
[2]  
Baker M., 2004, DTRS5602D70036 OFF P
[3]  
BEAVERS JA, 2001, CORR 2001 NACE HOUST
[4]  
BEAVERS JA, 1998, CORR 98 NACE INT HOU
[5]   Research and Cracking Implications from an Assessment of Two Variants of Near-Neutral pH Crack Colonies in Liquid Pipelines [J].
Bouaeshi, W. ;
Ironside, S. ;
Eadie, R. .
CORROSION, 2007, 63 (07) :648-660
[6]   Effect of hydrostatic testing on ductile tearing of X-65 line pipe steel with stress corrosion cracks [J].
Brongers, MPH ;
Beavers, JA ;
Jaske, CE ;
Delanty, BS .
CORROSION, 2000, 56 (10) :1050-1058
[7]   Mechanism for hydrogen evolution reaction on pipeline steel in near-neutral pH solution [J].
Cheng, Y. F. ;
Niu, L. .
ELECTROCHEMISTRY COMMUNICATIONS, 2007, 9 (04) :558-562
[8]   Thermodynamically modeling the interactions of hydrogen, stress and anodic dissolution at crack-tip during near-neutral pH SCC in pipelines [J].
Cheng, Y. F. .
JOURNAL OF MATERIALS SCIENCE, 2007, 42 (08) :2701-2705
[9]  
*CHIN NAT STAND ST, 2007, T15970 GB CHIN NAT S
[10]   Effect of microstructure on the stress corrosion cracking of X-80 pipeline steel in diluted sodium bicarbonate solutions [J].
Gonzalez-Rodriguez, JG ;
Casales, M ;
Salinas-Bravo, VM ;
Albarran, JL ;
Martinez, L .
CORROSION, 2002, 58 (07) :584-590