The analysis of surface degradation on UV-treated epoxy/glass fiber by corona-charging properties

被引:11
作者
Lee, BS [1 ]
Motoyama, T
Ichikawa, K
Tabata, Y
Lee, DC
机构
[1] Inha Univ, Dept Elect Engn, Inchon, South Korea
[2] Natl Inst Ind Safety, Tokyo 204, Japan
关键词
UV; epoxy/glass fiber; corona-charging; electric double layer; thermodynamic reorientation;
D O I
10.1016/S0141-3910(99)00078-6
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
We tried to apply corona-charging properties to the analysis of polymer surface degradation and demonstrated the inter-correlation between electrostatic changes and chemical structures on the surface of UV-treated epoxy/glass fiber. It was possible to detect the change of surface energy states and chemical structures with the measurement of contact angle and ESCA spectrum. Also, the changes of electrostatic behaviors were found through the results of surface potential decay, polarity effects, and surface resistivity. Finally, we can conclude that the polymer surface degradation proceeds with the formation of electric double layer by electrostatic force and the reorientation by thermodynamic force on the polymer surface. Especially, it was very important to find out the change of electrostatic behaviors by applying corona-charging properties. (C) 1999 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:271 / 278
页数:8
相关论文
共 16 条
[1]  
CHAN CM, 1994, POLYM SURFACE MODIFI
[2]   CORONA DISCHARGE PROCESSES [J].
CHANG, JS ;
LAWLESS, PA ;
YAMAMOTO, T .
IEEE TRANSACTIONS ON PLASMA SCIENCE, 1991, 19 (06) :1152-1166
[3]  
Dusek K, 1985, EPOXY RESINS COMPOSI
[4]  
FRIEDRICH J, 1996, SURF COAT TECH, V98, P879
[5]   Accelerated ac degradation of impregnated PP films [J].
Gadoum, A ;
Gosse, B ;
Gosse, JP .
IEEE TRANSACTIONS ON DIELECTRICS AND ELECTRICAL INSULATION, 1995, 2 (06) :1075-1082
[6]  
GARBASSI F, 1994, POLYM SURFACE PHYSIC
[7]   ELECTRICAL-CONDUCTION AND CHEMICAL-STRUCTURE OF INSULATING POLYMERS [J].
IEDA, M ;
MIZUTANI, T ;
IKEDA, S .
IEEE TRANSACTIONS ON ELECTRICAL INSULATION, 1986, 21 (03) :301-306
[8]   Photo-degradation of polyethylene and polypropylene at slow strain-rate [J].
Kelly, CT ;
White, JR .
POLYMER DEGRADATION AND STABILITY, 1997, 56 (03) :367-383
[9]  
Ku C.C., 1987, ELECT PROPERTIES POL
[10]   Generation of energetic He atom beams by a pulsed positive corona discharge [J].
Lo, SY ;
Lobo, JD ;
Blumberg, S ;
Dibble, TS ;
Zhang, X ;
Tsao, CC ;
Okumura, M .
JOURNAL OF APPLIED PHYSICS, 1997, 81 (09) :5896-5904