The effects of particle size and distribution on the magnetic properties of coercive Sm(Co,Fe,Cu,Zr)(z) alloy powders for bonded magnet applications

被引:9
作者
Gong, W
Ma, BM
Bounds, CO
机构
[1] Rhône-Poulenc, Rare Earths and Gallium, CN 7500, Cranbury
关键词
D O I
10.1063/1.364625
中图分类号
O59 [应用物理学];
学科分类号
摘要
The microstructure of Sm(CobalFexCu0.08Zr0.03)(8.2), where x = 0.23, 0.26, and 0.28, in the as-cast state and after various processing stages has been examined by optical microscopy. The size of the 2:17 matrix phase was found to be approximately 100 mu m in the as-cast state. A slight increase in the size of the 2:17 matrix was observed after thermal processing. Subgrains of 10 to 20 mu m are present in the 2:17 matrix of the fully processed ingots. Powders with a mean particle size range of 3-300 mu m were found to exhibit a Gaussian distribution. A slight increase in intrinsic coercivity (H-ci) was observed when the mean particle size was decreased from 300 to 200 mu m and remained nearly constant for sizes ranging between 10 and 200 mu m. A significant decrease in H-ci was observed when powders were further reduced below 10 mu m. Similar trends were also observed for remanence (B-r), maximum energy product (BHmax), and squareness of the second quadrant demagnetization curve. The size of the subgrains was found to be critical to these properties. The H-ci of alloy powders with a high Fe content appeared to degrade more severely when reduced below 10 mu m. For a fixed mean particle size, alloy powders with a high Fe content also exhibited a less-square second quadrant demagnetization curve. A B-r of 9.2 kG, H-ci of 18 kOe, H-cb Of 7.4 kOe, BHmax of 19 MGOe, and a squareness ratio of 0.91 have been obtained on Sm(CobalFe0.23Cu0.08Zr0.03)(8.2). As expected for alloys with a higher Fe content, B-r of 11.3 kG, H-ci of 20 kOe, H-cb Of 8.1 kOe, BHmax of 25 MGOe, and a square ratio of 0.83 have been obtained on Sm(CobalFe0.28Cu0.08Zr0.03)(8.2). (C) 1997 American Institute of Physics.
引用
收藏
页码:5640 / 5642
页数:3
相关论文
共 5 条
[1]   A STUDY OF MAGNETIC HARDENING IN SM(CO0.69FE0.22CU0.07ZR0.02)7.22 [J].
HADJIPANAYIS, GC ;
YADLOWSKY, EJ ;
WOLLINS, SH .
JOURNAL OF APPLIED PHYSICS, 1982, 53 (03) :2386-2388
[2]   COERCIVE SM2CO17 POWDER FOR THE BONDED MAGNET APPLICATION [J].
LIU, WL ;
LIANG, YL ;
SCOTT, DW ;
MA, BM ;
BOUNDS, CO .
IEEE TRANSACTIONS ON MAGNETICS, 1995, 31 (06) :3686-3688
[3]   PHASE-TRANSFORMATION AT HIGH-TEMPERATURE AND COERCIVITY OF SM(CO,CU,FE,ZR)7-9 MAGNET ALLOYS [J].
MORITA, Y ;
UMEDA, T ;
KIMURA, Y .
IEEE TRANSACTIONS ON MAGNETICS, 1987, 23 (05) :2702-2704
[4]   A REVISED MODEL FOR THE METALLURGICAL BEHAVIOR OF 2-17-TYPE PERMANENT-MAGNET ALLOYS [J].
RAY, AE .
JOURNAL OF APPLIED PHYSICS, 1990, 67 (09) :4972-4974
[5]  
SHIMODA T, 1979, 4TH P INT WORKSH RAR, P335