Hydrogen adsorption in carbon nanostructures compared

被引:72
作者
Schimmel, HG
Nijkamp, G
Kearley, GJ
Rivera, A
de Jong, KP
Mulder, FM
机构
[1] Delft Univ Technol, Interfac Reactor Inst, NL-2629 JB Delft, Netherlands
[2] Univ Utrecht, Debye Inst, NL-3508 TB Utrecht, Netherlands
来源
MATERIALS SCIENCE AND ENGINEERING B-SOLID STATE MATERIALS FOR ADVANCED TECHNOLOGY | 2004年 / 108卷 / 1-2期
关键词
hydrogen adsorption; single walled nanotubes; physisorption; carbon; density functional calculations;
D O I
10.1016/j.mseb.2003.10.091
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Recent reports continue to suggest high hydrogen storage capacities for some carbon nanostructures due to a stronger interaction between hydrogen and carbon. Here the interaction of hydrogen with activated charcoal, carbon nanofibers, single walled carbon nanotubes (SWNT), and electron beam 'opened' SWNT are compared and shown to be similar. The storage capacity below 77 K of these materials correlates with the surface area of the material with the activated charcoal having the largest. SWNT and 'opened' SWNT have a relatively low accessible surface area due to bundling of the tubes. Pressure-temperature curves give the interaction potential, which was found to be approximate to 580 K or 50 meV in all samples, leading to significant adsorption below approximate to 50 K. Using the inelastic neutron scattering signal associated with rotation of the hydrogen molecule as a sensitive probe for the surroundings of the molecule, no difference was found between the hydrogen molecules adsorbed in the investigated materials. These combined spectroscopic and macroscopic results show that SWNT, nanofibers and activated carbons store molecular hydrogen due to their graphitic nature and not because they possess special morphologies. Results from a density functional theory computer calculation suggest molecular hydrogen bonding to an aromatic C-C bond of graphite, irrespective of the surface morphology farther away. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:124 / 129
页数:6
相关论文
共 21 条
[1]   Surface reconstructions and dimensional changes in single-walled carbon nanotubes [J].
Ajayan, PM ;
Ravikumar, V ;
Charlier, JC .
PHYSICAL REVIEW LETTERS, 1998, 81 (07) :1437-1440
[2]   Hydrogen storage in graphite nanofibers [J].
Chambers, A ;
Park, C ;
Baker, RTK ;
Rodriguez, NM .
JOURNAL OF PHYSICAL CHEMISTRY B, 1998, 102 (22) :4253-4256
[3]   High H2 uptake by alkali-doped carbon nanotubes under ambient pressure and moderate temperatures [J].
Chen, P ;
Wu, X ;
Lin, J ;
Tan, KL .
SCIENCE, 1999, 285 (5424) :91-93
[4]  
De Boer JH., 1968, DYNAMICAL CHARACTER
[5]   Storage of hydrogen in single-walled carbon nanotubes [J].
Dillon, AC ;
Jones, KM ;
Bekkedahl, TA ;
Kiang, CH ;
Bethune, DS ;
Heben, MJ .
NATURE, 1997, 386 (6623) :377-379
[6]  
Du WF, 2002, NANO LETT, V2, P343, DOI [10.1021/nl010096a, 10.1021/n1010096a]
[7]   A study of micropores in single-walled carbon nanotubes by the adsorption of gases and vapors [J].
Eswaramoorthy, M ;
Sen, R ;
Rao, CNR .
CHEMICAL PHYSICS LETTERS, 1999, 304 (3-4) :207-210
[8]   Spin-echo small-angle neutron scattering to study particle aggregates [J].
Krouglov, T ;
Kraan, WH ;
Plomp, J ;
Rekveldt, MT ;
Bouwman, WG .
JOURNAL OF APPLIED CRYSTALLOGRAPHY, 2003, 36 :816-819
[9]   Coordination of palladium on carbon fibrils as determined by XAFS spectroscopy [J].
Mojet, BL ;
Hoogenraad, MS ;
van Dillen, AJ ;
Geus, JW ;
Koningsberger, DC .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS, 1997, 93 (24) :4371-4375
[10]   Dynamics of a triphenylene discotic molecule, HAT6, in the columnar and isotropic liquid phases [J].
Mulder, FM ;
Stride, J ;
Picken, SJ ;
Kouwer, PHJ ;
de Haas, MP ;
Siebbeles, LDA ;
Kearley, GJ .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2003, 125 (13) :3860-3866