Deodorant properties of wool fabrics dyed with acid mordant dyes and a copper salt

被引:25
作者
Kobayashi, Y [1 ]
Nakanishi, T
Komiyama, J
机构
[1] Tokyo Kasei Jr Coll, Itabashi Ku, Tokyo 1738602, Japan
[2] Jissen Womens Univ, Dept Human Environm Sci, Tokyo 1918510, Japan
关键词
D O I
10.1177/004051750207200206
中图分类号
TB3 [工程材料学]; TS1 [纺织工业、染整工业];
学科分类号
0805 ; 080502 ; 0821 ;
摘要
Wool fabrics with a deodorant function are prepared by acid mordant dyeing with copper(II) nitrate. The effects of pre- and after-mordanting are examined for C.I. Mordant Yellow 3 and C.I. Mordant Red 17. Carboxylate groups in the wool fibers and the dyes work to fix copper ion with the deodorant ability against mercaptan. The elimination of mercaptan from the air by the mordant dyed fabrics is measured in a Teddler bag. Fabrics untreated or dyed without mordanting show no deodorant ability, but those pre-mordanted or pre- and after-mordanted show considerable deodorant ability. By controlling the pH of the dyebath to about 4, dye and copper ion uptake of the fabric is optimized and the deodorant ability is also optimum.
引用
收藏
页码:125 / 131
页数:7
相关论文
共 17 条
[1]  
AMEMIYA T, 1999, SEN I GAKKAI PREPRIN, pG81
[2]   Iron salts in the post-metallization of mordant dyes [J].
Bardole, HA ;
Freeman, HS ;
Reife, A .
TEXTILE RESEARCH JOURNAL, 1998, 68 (02) :141-149
[3]  
Baughman GL, 2000, TEXT CHEM COLOR AM D, V32, P51
[4]  
Etters JN, 1999, TEXT CHEM COLOR AM D, V1, P33
[5]  
JURIA MR, 1993, MELLIAND TEXTILBER, V74, P1161
[6]  
KUWAHARA S, 1993, JPN RES ASS TEXTILE, V34, P301
[7]  
NAKASHIMA T, 1998, DYEING IND, V46, P205
[8]  
*NOV CO, 1997, CHEM FIBERS INT, V47, P367
[9]  
Parton K, 1998, J SOC DYERS COLOUR, V114, P8
[10]  
*RES GROUP POL COM, 1991, BIOM COMPL, P281