Effect of water on the low temperature conductivity of polymer electrolytes

被引:151
作者
Siu, A [1 ]
Schmeisser, J [1 ]
Holdcroft, S [1 ]
机构
[1] Natl Res Council Canada, Inst Fuel Cell Innovat, Vancouver, BC V6T 1W5, Canada
关键词
D O I
10.1021/jp0531208
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The proton conductivity of radiation-grafted ethylenetetrafluoroethylene-grafted-poly(styrene sulfonic) acid (ETFE-g-PSSA) and Nafion 117 membranes between 25 and -37 degrees C is reported. The freezing of water in the membranes, which strongly depends on the internal acid concentration, results in a 4-fold decrease in proton conductivity. The activation energies before and after the freezing of the membranes are similar to 0.15 and 0.4 eV, consistent with proton transport through liquid water and strongly bound water, respectively. Differential scanning calorimetry data show that up to 14 H2O molecules per H+/SO3- group remain unfrozen at subzero temperatures and are believed to be responsible for the low temperature conductivity that is observed. These results indicate that proton conductivity in membranes may be achieved via strongly bound and highly polarized water.
引用
收藏
页码:6072 / 6080
页数:9
相关论文
共 39 条
[1]   Polymeric proton conducting membranes for medium temperature fuel cells (110-160°C) [J].
Alberti, G ;
Casciola, M ;
Massinelli, L ;
Bauer, B .
JOURNAL OF MEMBRANE SCIENCE, 2001, 185 (01) :73-81
[2]   Studies on ion-exchange membranes .1. Effect of humidity on the conductivity of Nafion(R) [J].
Anantaraman, AV ;
Gardner, CL .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1996, 414 (02) :115-120
[3]  
Atkins JR, 2003, J NEW MAT ELECTR SYS, V6, P9
[4]  
ATKINS P, 1999, PHYS CHEM, P723
[5]   Ionic conductivity of proton exchange membranes [J].
Beattie, PD ;
Orfino, FP ;
Basura, VI ;
Zychowska, K ;
Ding, JF ;
Chuy, C ;
Schmeisser, J ;
Holdcroft, S .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 2001, 503 (1-2) :45-56
[6]   CONDUCTANCE OF NAFION-117 MEMBRANES AS A FUNCTION OF TEMPERATURE AND WATER-CONTENT [J].
CAPPADONIA, M ;
ERNING, JW ;
NIAKI, SMS ;
STIMMING, U .
SOLID STATE IONICS, 1995, 77 :65-69
[7]   PROTON CONDUCTION OF NAFION((R))-117 MEMBRANE BETWEEN 140 K AND ROOM-TEMPERATURE [J].
CAPPADONIA, M ;
ERNING, JW ;
STIMMING, U .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1994, 376 (1-2) :189-193
[8]   Electrochemical characterization of ethylenetetrafluoroethylene-g-polystyrenesulfonic acid solid polymer electrolytes [J].
Chuy, C ;
Basura, VI ;
Simon, E ;
Holdcroft, S ;
Horsfall, J ;
Lovell, KV .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2000, 147 (12) :4453-4458
[9]   Solid state 1H NMR study, humidity sensitivity and protonic conduction of gel derived phosphosilicate glasses [J].
Clayden, NJ ;
Esposito, S ;
Pernice, P ;
Aronne, A .
JOURNAL OF MATERIALS CHEMISTRY, 2002, 12 (12) :3746-3753
[10]  
Colomban P., 1992, PROTON CONDUCTORS SO, P38