Scanning probe microscope observations of fatigue process in magnesium alloy AZ31 near the fatigue limit

被引:35
作者
Nan, ZY [1 ]
Ishihara, S [1 ]
Goshima, T [1 ]
Nakanishi, R [1 ]
机构
[1] Toyama Univ, Dept Mech Engn, Toyama 9308555, Japan
关键词
magnesium alloy; scanning probe microscope; fatigue; crack initiation; crack propagation;
D O I
10.1016/j.scriptamat.2003.11.007
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
In this study, fatigue crack initiation and propagation behavior of magnesium alloy AZ31 within a crystal grain near the fatigue limit were investigated in detail using a scanning probe microscope (SPM). At a stress amplitude slightly higher than the fatigue limit, cracks are arrested by the grain boundary for an extended period. (C) 2003 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
引用
收藏
页码:429 / 434
页数:6
相关论文
共 7 条
[1]   Cyclic deformation and fatigue behaviour of the magnesium alloy AZ91 [J].
Eisenmeier, G ;
Holzwarth, B ;
Höppel, HW ;
Mughrabi, H .
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, 2001, 319 :578-582
[2]  
Kojima Y., 2000, HDB ADV MAGNESIUM TE
[3]  
NAKAI Y, 1999, T JAPAN SOC MECH E A, V65, P483
[4]  
NAN ZY, UNPUB T JPN SOC ME A
[5]  
Ohgi J, 1998, EXPERIMENTAL MECHANICS, VOLS 1 AND 2, P1053
[6]  
SAJURI ZB, 2002, P 8 INT FAT C FAT 20, P3301
[7]  
YUN WG, 1998, T JPN SOC MECH ENG A, V64, P1435