Electrooxidation of stainless steel AISI 304 in carbonate aqueous solution at pH8

被引:28
作者
Drogowska, M [1 ]
Menard, H [1 ]
Brossard, L [1 ]
机构
[1] INST RECH HYDRO QUEBEC, IREQ, VARENNES, PQ J3X 1S1, CANADA
关键词
D O I
10.1007/BF00364073
中图分类号
O646 [电化学、电解、磁化学];
学科分类号
081704 ;
摘要
The electrochemical behaviour of stainless steel AISI 304 (SS304) has been investigated in deaerated 0.1-1M NaHCO3 solutions at pH 8 using a rotating disc electrode. The polarization curves are characterized by a broad range of passivity at low potentials (-0.8 to 0.3 V), a depassivation region at 0.4 V vs SCE and, at high potentials (0.5 to 0.85 V), a passive region before oxygen evolution. In the low potential range, the SS304 electrode behaves like a Cr-rich metallic phase, and the dissolution of Fe2+ ions into the solution is hindered by the formation of a Cr2O3 layer. As the potential reaches 0.4 V, the oxidation-dissolution of Cr(III) oxide/hydroxide to CrO42- ions occurs, with the participation of bicarbonate/carbonate as a catalyst in the dissolution reaction. Since the chromium oxide/hydroxide dissolution and subsequent surface enrichment ofiron oxides occur, the applied potential, exposure time and oxidation charge have a considerable effect on the passive him properties. At high potentials, the presence of a passive him of iron oxides/hydroxides or oxyhydroxides plays a key role in the SS304 passivity with the presence of Fe(VI) species incorporated or adsorbed into the passive films. Colouration of the SS304 surface is observed in the second passive region. A him of a uniform gold colour formed on SS304, mild steel 1024 and iron in carbonate and.borate solutions at pH 8. The colour of the electrode surfaces remain unchanged in air and in solutions at positive potential but it disappears at open-circuit potential or is easily reduced in the first negative-going potential scan.
引用
收藏
页码:217 / 225
页数:9
相关论文
共 56 条
[1]  
[Anonymous], 1964, SPECIAL PUBLICATION
[2]   SEMICONDUCTING PROPERTIES OF PASSIVE FILMS ON AISI-304 AND AISI-316 STAINLESS-STEELS [J].
BABIC, R ;
METIKOSHUKOVIC, M .
JOURNAL OF ELECTROANALYTICAL CHEMISTRY, 1993, 358 (1-2) :143-160
[3]  
Bard A. J., 1985, STANDARD POTENTIALS, P453
[4]   NATURE OF THE PASSIVE FILM ON FE-CR ALLOYS AS STUDIED BY O-18 SECONDARY ION MASS-SPECTROMETRY - REDUCTION OF THE PRIOR FILM AND STABILITY TO EXSITU SURFACE-ANALYSIS [J].
BARDWELL, JA ;
SPROULE, GI ;
MITCHELL, DF ;
MACDOUGALL, B ;
GRAHAM, MJ .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS, 1991, 87 (07) :1011-1019
[5]   INSITU XANES DETECTION OF CR(VI) IN THE PASSIVE FILM ON FE-26CR [J].
BARDWELL, JA ;
SPROULE, GI ;
MACDOUGALL, B ;
GRAHAM, MJ ;
DAVENPORT, AJ ;
ISAACS, HS .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1992, 139 (02) :371-373
[6]   TRANSPASSIVE DISSOLUTION OF IRON TO FERRATE (VI) IN CONCENTRATED ALKALI HYDROXIDE SOLUTIONS [J].
BECK, F ;
KAUS, R ;
OBERST, M .
ELECTROCHIMICA ACTA, 1985, 30 (02) :173-183
[7]   THE ELECTROCHEMISTRY OF CHROMIUM IN ACIDIC CHLORIDE SOLUTIONS - ANODIC-DISSOLUTION AND PASSIVATION [J].
BJORNKVIST, L ;
OLEFJORD, I .
CORROSION SCIENCE, 1991, 32 (02) :231-242
[8]   ON THE ROLE OF CR IN THE PASSIVITY OF STAINLESS-STEEL [J].
BROOKS, AR ;
CLAYTON, CR ;
DOSS, K ;
LU, YC .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1986, 133 (12) :2459-2464
[9]   ISS DEPTH PROFILES OF THE PASSIVE LAYER ON FE/CR ALLOYS [J].
CALINSKI, C ;
STREHBLOW, HH .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1989, 136 (05) :1328-1331
[10]   A POINT-DEFECT MODEL FOR ANODIC PASSIVE FILMS .3. IMPEDANCE RESPONSE [J].
CHAO, CY ;
LIN, LF ;
MACDONALD, DD .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1982, 129 (09) :1874-1879