Improved photoluminescence of BaMgAl10O17 blue phosphor prepared by spray pyrolysis

被引:47
作者
Jung, KY [1 ]
Lee, DY [1 ]
Kang, YC [1 ]
Park, HD [1 ]
机构
[1] Korea Res Inst Chem Technol, Adv Mat Div, Taejon 305600, South Korea
关键词
phosphor; spray pyrolysis; blue phosphor; photoluminescence;
D O I
10.1016/S0022-2313(03)00118-2
中图分类号
O43 [光学];
学科分类号
070207 ; 0803 ;
摘要
BaMgAl10O17:Eu2+ (BAM) blue phosphor particles with improved photoluminescence (PL) intensity under vacuum ultraviolet (VUV) excitation were prepared by a spray pyrolysis process. In order to improve the PL intensity, Er3+ and Nd3+ ions were used as co-doping elements. The VUV characteristics of BAM:Eu2+, M+ (M = Er, Nd) were monitored with varying the Er3+ and Nd3+ content in order to find the optimal co-doping concentration when they were prepared by spray pyrolysis. It was found that doping Er3+ or Nd3+ enhances the PL intensity of BAM:Eu2+ blue phosphor particles. In particular, the M3+ doping effect on the PL intensity was pronounced when the prepared BAM:Eu2+, M3+ particles were excited by 172 nm VUV. The maximum intensity was obtained when the M3+ content was 1.0 at% with respect to Ba element. The PL intensity of BAM:Eu2+,M+ (M = Er3+, Nd3+) particles was also further improved by producing them in a spherical shape, which was successfully achieved by controlling the spray solution. The optimized BAM:Eu2+,M+ particles had about 10% higher PL intensity than that of the commercial particles, which are made by a conventional solid-state reaction. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:127 / 133
页数:7
相关论文
共 24 条
[1]   Low-temperature synthesis of pure and Mn-doped willemite phosphor (Zn2SiO4:Mn) in aqueous medium [J].
Ahmadi, TS ;
Haase, M ;
Weller, H .
MATERIALS RESEARCH BULLETIN, 2000, 35 (11) :1869-1879
[2]  
AHONEN P, 1996, J AERSOL SCI, V27, pS373
[3]  
Bhatkar VB, 2002, PHYS STATUS SOLIDI A, V191, P272, DOI 10.1002/1521-396X(200205)191:1<272::AID-PSSA272>3.0.CO
[4]  
2-R
[5]  
BRINKER CJ, 1990, SOL GEL SCI PHYSICS
[6]  
GURAV AS, 1995, J AEROSOL SCI, V26, pS833
[7]   Morphology control of BaMgAl10O17:Eu particles:: The use of colloidal solution obtained from alkoxide precursor in spray pyrolysis [J].
Kang, KC ;
Park, SB .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2000, 147 (02) :799-802
[8]   Y2SiO5:Ce phosphor particles 0.5-1.4 μm in size with spherical morphology [J].
Kang, YC ;
Lenggoro, IW ;
Park, SB ;
Okuyama, K .
JOURNAL OF SOLID STATE CHEMISTRY, 1999, 146 (01) :168-175
[9]   Zn2SiO4:Mn phosphor particles prepared by spray pyrolysis using a filter expansion aerosol generator [J].
Kang, YC ;
Park, SB .
MATERIALS RESEARCH BULLETIN, 2000, 35 (07) :1143-1151
[10]   The effect of metal chloride fluxes on the properties of phosphor particles in spray pyrolysis [J].
Kang, YC ;
Park, HD ;
Park, SB .
JAPANESE JOURNAL OF APPLIED PHYSICS PART 2-LETTERS, 2000, 39 (12B) :L1305-L1307