Polydimethylsiloxane thermal degradation - Part 1. Kinetic aspects

被引:707
作者
Camino, G [1 ]
Lomakin, SM [1 ]
Lazzari, M [1 ]
机构
[1] Univ Turin, Dipartimento Chim Inorgan Chim Fis & Chim Mat, I-10125 Turin, Italy
关键词
depolymerization of polysiloxanes; kinetics of depolymerization; thermal degradation;
D O I
10.1016/S0032-3861(00)00652-2
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
A combination of traditional kinetic formal treatments and computer simulation has been made to analyze polydimethylsiloxane (PDMS) thermal degradation. It was shown that PDMS thermally decomposes to cyclic oligomers through Si-O bond scission in a chain-folded cyclic conformation energetically favored by overlapping of empty silicon d-orbitals with orbitals of oxygen and carbon atoms. Kinetic treatment shows that PDMS thermal volatilization, as rate of heating increases, becomes dominated by rate of diffusion and evaporation of oligomers produced on its decomposition. At high heating rate (e.g. 100 degreesC min(-1).) thermal decomposition in nitrogen and in air tend to overlap because the rate of reaction between the material and oxygen is strongly reduced by low-oxygen solubility and high-thermal degradation rate. In nitrogen a small black residue is formed (silicon oxycarbide) which is produced by an alternative decomposition path leading to cyclic oligomers, made possible at high heating rate. (C) 2000 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2395 / 2402
页数:8
相关论文
共 16 条
[1]  
ANDRIANOV KA, 1971, VYSOKOMOL SOEDIN A, V14, P253
[2]   SIMPLE KINETIC MODELS FROM ARRHENIUS TO COMPUTER [J].
BUNKER, DL .
ACCOUNTS OF CHEMICAL RESEARCH, 1974, 7 (06) :195-201
[3]   HIGH-TEMPERATURE CHEMISTRY OF THE CONVERSION OF SILOXANES TO SILICON-CARBIDE [J].
BURNS, GT ;
TAYLOR, RB ;
XU, YR ;
ZANGVIL, A ;
ZANK, GA .
CHEMISTRY OF MATERIALS, 1992, 4 (06) :1313-1323
[4]   SI-29 NUCLEAR-MAGNETIC-RESONANCE STUDY OF THE STRUCTURE OF SILICON OXYCARBIDE GLASSES DERIVED FROM ORGANOSILICON PRECURSORS [J].
CORRIU, RJP ;
LECLERCQ, D ;
MUTIN, PH ;
VIOUX, A .
JOURNAL OF MATERIALS SCIENCE, 1995, 30 (09) :2313-2318
[5]   PEROXIDES .8. THE MECHANISM FOR THE THERMAL DECOMPOSITION OF NORMAL-BUTYL HYDROPEROXIDE AND NORMAL-BUTYL 1-HYDROXYBUTYL PEROXIDE [J].
DURHAM, LJ ;
WURSTER, CF ;
MOSHER, HS .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1958, 80 (02) :332-337
[6]   BULK SEMICONDUCTORS FROM MOLECULAR-SOLIDS - A MECHANISTIC INVESTIGATION [J].
FARNETH, WE ;
HERRON, N ;
WANG, Y .
CHEMISTRY OF MATERIALS, 1992, 4 (04) :916-922
[7]   THERMAL-DEGRADATION OF POLYSILOXANES .1. POLY(DIMETHYLSILOXANE) [J].
GRASSIE, N ;
MACFARLANE, IG .
EUROPEAN POLYMER JOURNAL, 1978, 14 (11) :875-884
[8]   COMPARISONS BETWEEN FULLERENE AND FORMS OF WELL-KNOWN CARBONS [J].
ISMAIL, IMK ;
RODGERS, SL .
CARBON, 1992, 30 (02) :229-239
[9]  
KISSINGER HE, 1957, ANAL CHEM, V29, P1702, DOI DOI 10.1021/AC60131A045
[10]  
KORSHAK VV, 1971, CHEM STRUCTURE THERM