Effect of nickel-titanium shape memory metal alloy on bone formation

被引:100
作者
Kapanen, A
Ryhänen, J
Danilov, A
Tuukkanen, J
机构
[1] Univ Oulu, Bioctr, FIN-90014 Oulu, Finland
[2] Univ Oulu, Dept Anat & Cell Biol, FIN-90014 Oulu, Finland
[3] Univ Oulu, Dept Surg, FIN-90014 Oulu, Finland
关键词
nitinol; biocompatibility; ectopic bone formation assay; PQCT; decalcified bone matrix;
D O I
10.1016/S0142-9612(00)00435-X
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
The aim of this study was to determine the biocompatibility of NiTi alloy on bone formation in vivo. For this purpose we used ectopic bone formation assay which goes through all the events of bone formation and calcification. Comparisons were made between Nitinol (NiTi), stainless steel (Stst) and titanium-aluminium (6%)-vanadium (4%) alloy (Ti-6Al-4V), which were implanted for 8 weeks under the fascia of the latissimus dorsi muscle in 3-month-old rats. A light-microscopic examination showed no chronic inflammatory or other pathological findings in the induced ossicle or its capsule. New bone replaced part of the decalcified matrix with mineralized new cartilage and bone. The mineral density was measured with peripheral quantitative computed tomography (pQCT). The total bone mineral density (BMD) values were nearly equal between the control and the NiTi samples, the Stst samples and the Ti-6Al-4V samples had lower BMDs. Digital image analysis was used to measure the combined area of new fibrotic tissue and original implanted bone matrix powder around the implants. There were no significant differences between the implanted materials, although Ti-6Al-4V showed the largest matrix powder areas. The same method was used for measurements of proportional cartilage and new bone areas in the ossicles. NiTi showed the largest cartilage area (p less than or equal to 0.05). Between implant groups the new bone area was largest in NiTi. We conclude that NiTi has good biocompatibility, as its effects on ectopic bone formation are similar to those of Stst, and that the ectopic bone formation assay developed here can be used for biocompatibility studies. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:2475 / 2480
页数:6
相关论文
共 37 条
[1]   THE ROLE OF CELLS VERSUS MATRIX IN BONE INDUCTION [J].
ANDERSON, HC .
CONNECTIVE TISSUE RESEARCH, 1990, 24 (01) :3-12
[2]  
Assad M, 1999, BIO-MED MATER ENG, V9, P1
[3]   Quantitative assessment of experimental fracture repair by peripheral computed tomography [J].
Augat, P ;
Merk, J ;
Genant, HK ;
Claes, L .
CALCIFIED TISSUE INTERNATIONAL, 1997, 60 (02) :194-199
[4]  
Baumgart F., 1980, CURRENT CONCEPTS INT, P122
[5]  
BergerGorbet M, 1996, J BIOMED MATER RES, V32, P243, DOI 10.1002/(SICI)1097-4636(199610)32:2<243::AID-JBM14>3.0.CO
[6]  
2-K
[7]   Endoluminal stent-grafts for infrarenal abdominal aortic aneurysms [J].
Blum, U ;
Voshage, G ;
Lammer, J ;
Beyersdorf, F ;
Tollner, D ;
Kretschmer, G ;
Spillner, G ;
Polterauer, P ;
Nagel, G ;
Holzenbein, T ;
Thurnher, S ;
Langer, M .
NEW ENGLAND JOURNAL OF MEDICINE, 1997, 336 (01) :13-20
[8]   INVITRO MODEL OF ALUMINUM-INDUCED OSTEOMALACIA - INHIBITION OF HYDROXYAPATITE FORMATION AND GROWTH [J].
BLUMENTHAL, NC ;
POSNER, AS .
CALCIFIED TISSUE INTERNATIONAL, 1984, 36 (04) :439-441
[9]  
Buehler W.J., 1968, Ocean Eng, V1, P105, DOI [DOI 10.1016/0029-8018(68)90019-X, 10.1016/0029-8018(68)90019-X]
[10]   BIOCOMPATIBILITY OF NITINOL ALLOY AS AN IMPLANT MATERIAL [J].
CASTLEMAN, LS ;
MOTZKIN, SM ;
ALICANDRI, FP ;
BONAWIT, VL ;
JOHNSON, AA .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 1976, 10 (05) :695-731