Characterisation of low molar mass siloxanes extracted from crosslinked polydimethylsiloxanes exposed to corona discharges

被引:47
作者
Hillborg, H
Karlsson, S
Gedde, UW [1 ]
机构
[1] Royal Inst Technol, Dept Polymer Technol, SE-10044 Stockholm, Sweden
[2] ABB Corp Res, Dept High Voltage Engn, SE-72178 Vasteras, Sweden
关键词
polydimethylsiloxane; corona discharges; degradation products;
D O I
10.1016/S0032-3861(01)00451-7
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Crosslinked polydimethylsiloxanes were exposed to corona discharges in dry air at normal pressure. Short-time solvent extraction and subsequent analysis of the extractables, by gas chromatography, mass spectrometry and size exclusion chromatography showed that, oligomers consisting mainly of cyclics with 4-9 repeating units were formed during corona exposure. The size distribution of the oligomers was independent of the crosslink density and corona exposure time. The amount of oligomers located at the surface increased, with increasing storage time, after the corona exposure in qualitative agreement with the ongoing hydrophobic recovery process. Longer extractions penetrated deeper into the samples, and, in addition to the cyclic oligomers, higher molar mass species (similar to 50,000 g mol(-1) for unexposed samples) were detected. Samples exposed to corona, treated in this way, showed a broadening of the high molar mass peak towards lower molar masses. (C) 2001 Elsevier Science Ltd. All rights reserved.
引用
收藏
页码:8883 / 8889
页数:7
相关论文
共 30 条
[1]  
[Anonymous], [No title captured]
[2]  
BANNISTER DJ, 1981, POLYMER, V22, P337
[3]   THERMAL-DECOMPOSITION OF CYCLO-LINEAR METHYLSILOXANE POLYMERS [J].
BLAZSO, M ;
GARZO, G ;
ANDRIANOV, KA ;
MAKAROVA, NN ;
CHERNAVSKI, AI ;
PETROV, IM .
JOURNAL OF ORGANOMETALLIC CHEMISTRY, 1979, 165 (03) :273-279
[4]  
BLAZSO M, 1972, CHROMATOGRAPHIA, V5, P485
[5]   Characterization of poly(dimethylsiloxane)s by time-of-flight secondary ion mass spectrometry [J].
Dong, X ;
Proctor, A ;
Hercules, DM .
MACROMOLECULES, 1997, 30 (01) :63-70
[6]   LOGARITHMIC THERMAL DEGRADATION OF A SILICONE RESIN IN AIR [J].
DOYLE, CD .
JOURNAL OF POLYMER SCIENCE, 1958, 31 (122) :95-104
[7]   A new determination of the molecular dimensions [J].
Einstein, A .
ANNALEN DER PHYSIK, 1906, 19 (02) :289-306
[8]   MACROCYCLIZATION EQUILIBRIUM CONSTANTS AND STATISTICAL CONFIGURATION OF POLY(DIMETHYLSILOXANE) CHAINS [J].
FLORY, PJ ;
SEMLYEN, JA .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1966, 88 (14) :3209-&
[9]   POLYORGANOSILOXANES .... SURFACE ACTIVE PROPERTIES [J].
FOX, HW ;
TAYLOR, PW ;
ZISMAN, WA .
INDUSTRIAL AND ENGINEERING CHEMISTRY, 1947, 39 (11) :1401-1409
[10]   Hydrophobic recovery of plasma-treated polydimethylsiloxane [J].
Fritz, JL ;
Owen, MJ .
JOURNAL OF ADHESION, 1995, 54 (1-2) :33-45