Thermo-oxidative degradation of siloxane-containing polyimide and unmodified polyimide

被引:26
作者
Chang, TC [1 ]
Wu, KH
Liao, CL
Lin, ST
Wang, GP
机构
[1] Chung Cheng Inst Technol, Dept Appl Chem, Tao Yuan 33509, Taiwan
[2] Chung Shan Inst Sci & Technol, Chem Syst Res Div, Lungtan 32526, Taiwan
关键词
D O I
10.1016/S0141-3910(98)00011-1
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Five methods were used to study the thermo-oxidative degradation of siloxane-containing polyimide (polysiloxaneimide, PSI), and the results were compared with unmodified polyimide. The degradation of PSI was found to be a complex process composed of at least two overlapping stages for which apparent activation energies can be calculated. These investigated methods were those of Kissinger, Van Krevelen, Horowitz-Metzger, Coats-Redfern, and MacCallum-Tanner. These methodologies evaluated the different apparent activation energies E-a, and the single heating rate techniques proved more precise. The E-a of the imide segments in PSI was larger than that in PI. The result may be rationalized on the basis of the formation of thermally stable structures. (C) 1998 Elsevier Science Limited. All rights reserved.
引用
收藏
页码:299 / 305
页数:7
相关论文
共 19 条
  • [1] STRUCTURE PROPERTY BEHAVIOR OF SOLUBLE POLYIMIDE POLYDIMETHYLSILOXANE SEGMENTED COPOLYMERS
    ARNOLD, CA
    SUMMERS, JD
    CHEN, YP
    BOTT, RH
    CHEN, D
    MCGRATH, JE
    [J]. POLYMER, 1989, 30 (06) : 986 - 995
  • [2] Chang TC, 1996, J POLYM SCI POL CHEM, V34, P3337, DOI 10.1002/(SICI)1099-0518(19961130)34:16<3337::AID-POLA10>3.0.CO
  • [3] 2-H
  • [4] The effect of silicon and phosphorus on the degradation of poly(methyl methacrylate)
    Chang, TC
    Chen, YC
    Ho, SY
    Chiu, YS
    [J]. POLYMER, 1996, 37 (14) : 2963 - 2968
  • [5] Characterization and degradation of some silicon-containing polyimides
    Chang, TC
    Wu, KH
    [J]. POLYMER DEGRADATION AND STABILITY, 1998, 60 (01) : 161 - 168
  • [6] THERMOOXIDATIVE DEGRADATION OF PHOSPHORUS-CONTAINING POLYURETHANE
    CHANG, TC
    SHEN, WS
    CHIU, YS
    HO, SY
    [J]. POLYMER DEGRADATION AND STABILITY, 1995, 49 (03) : 353 - 360
  • [7] Clarson S. J., 1993, SILOXANE POLYM, P72
  • [8] KINETIC PARAMETERS FROM THERMOGRAVIMETRIC DATA
    COATS, AW
    REDFERN, JP
    [J]. NATURE, 1964, 201 (491) : 68 - &
  • [9] THERMOGRAVIMETRIC ANALYSIS STUDY OF THE MECHANISM OF PYROLYSIS OF UNTREATED AND FLAME-RETARDANT TREATED COTTON FABRICS UNDER A CONTINUOUS-FLOW OF NITROGEN
    FAROQ, AA
    PRICE, D
    MILNES, GJ
    HORROCKS, AR
    [J]. POLYMER DEGRADATION AND STABILITY, 1994, 44 (03) : 323 - 333
  • [10] GREBER G, 1968, ANG MAKROMOL CHEM, V4, P212