Influence of ceramic surface treatment on peel-off strength between aluminum nitride and epoxy-modified polyaminobismaleimide adhesive

被引:20
作者
Asai, H [1 ]
Iwase, N
Suga, T
机构
[1] Toshiba Corp, Ctr Corp Res & Dev, Display Mat & Devices Lab, Kawasaki, Kanagawa 2128582, Japan
[2] Univ Tokyo, Res Ctr Adv Sci & Technol, Tokyo 1538904, Japan
来源
IEEE TRANSACTIONS ON ADVANCED PACKAGING | 2001年 / 24卷 / 01期
关键词
adhesive; aluminum nitride; chemical state; peel-off strength; polyaminobismaleimide; surface free energy; surface shape; surface treatment;
D O I
10.1109/6040.909633
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
Peel-off strength between aluminum nitride (AlN) ceramics and a polyaminobismaleimide (PABM) adhesive is investigated after surface treatments. The surface treatments of the AIN substrates were oxygen plasma exposure, K2O .n(B2O3) aqueous solution immersion and a combination of the two. Each of the three methods increases the peel-off strength compared to that in the case of no surface treatment. In the case of the combination of oxygen plasma exposure for 60 s and K2O .n(B2O3) aqueous solution immersion for 10 min, average peel-off strength was over 1.6 N/mm, whereas that in the case of no surface treatment was 0.14 N/mm, Oxygen plasma exposure and K2O .n(B2O3) aqueous solution immersion decreased the relative amounts of carbon and hydrocarbon on the surface of as-sintered AIN substrates, On the other hand, the relative amount of hydrophilic groups, such as COO, C=O, and C-O relatively increased, This chemical change is effective for increasing peel-off strength. The results of measurement of surface free energy of the AIN substrate surface indicate that these surface treatments increase surface energy of AIN substrates from about 47 to 60 mJ/m(2), When AIN substrate was immersed in K2O .n(B2O3) aqueous solution, tiny protrusions were formed on the AIN grain surfaces, The approximate height and pitch of the protrusions were about 30 nm and 60 nm, respectively, in the case of immersion for 10 min. Most AIN grains were etched, although no all. This change in shape of grains to brings about resistance to peeling and contributes to enlargement of the surface area. Due to these effects, average peel-off strength of AIN substrates with both oxygen plasma exposure and K2O .n(B2O3) aqueous solution immersion was 1.1 N/mm even after 800 cycles of thermal cycling and the value is still larger than that required for the practical package application.
引用
收藏
页码:104 / 112
页数:9
相关论文
共 16 条
[1]   Design and characteristics of a newly developed cavity-up plastic and ceramic laminated thin BGA package [J].
Asai, H ;
Yano, K ;
Iyogi, K ;
Iwase, N ;
Fujiwara, T .
IEEE TRANSACTIONS ON ADVANCED PACKAGING, 1999, 22 (03) :460-467
[2]   Influence of the grain boundary phase on the mechanical strength at aluminum nitride substrate surfaces [J].
Asai, H ;
Takahashi, T .
IEEE TRANSACTIONS ON ADVANCED PACKAGING, 2000, 23 (03) :452-460
[3]  
ASAI H, 2000, J JPN I ELECT PACKAG, V3, P494
[4]   EXTENDED DEFECTS IN SINTERED AIN [J].
DENANOT, MF ;
RABIER, J .
JOURNAL OF MATERIALS SCIENCE, 1989, 24 (05) :1594-1598
[5]  
DOI K, 1995, P INT S MICR OCT, P247
[6]  
HARRIS JH, 1990, J MAT RES AUG, V5
[7]  
HERCZEG A, 1970, P NAT SAMPE TECH C, V2, P221
[8]   DIFFUSE-REFLECTANCE FOURIER-TRANSFORM INFRARED SPECTROSCOPIC STUDIES OF THE STABILITY OF ALUMINUM NITRIDE POWDER IN AN AQUEOUS ENVIRONMENT [J].
HIGHFIELD, JG ;
BOWEN, P .
ANALYTICAL CHEMISTRY, 1989, 61 (21) :2399-2402
[9]   HYDROPHOBING OF ALUMINUM NITRIDE POWDERS [J].
HOTZA, D ;
SAHLING, O ;
GREIL, P .
JOURNAL OF MATERIALS SCIENCE, 1995, 30 (01) :127-132
[10]  
IKADA Y, 1979, J ADHESION SOC JPN, V15, P91