Photo-cross-linkable polymers having degradable properties on heating

被引:56
作者
Shirai, M [1 ]
Kawaue, A [1 ]
Okamura, H [1 ]
Tsunooka, M [1 ]
机构
[1] Osaka Prefecture Univ, Grad Sch Engn, Dept Appl Chem, Sakai, Osaka 5998531, Japan
关键词
D O I
10.1021/cm0302734
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Photo-cross-linkable polymers having degradable properties on heating were described. Copolymers of esters or salts of p-styrenesulfonic acid with a novel monomer having both an epoxy moiety and a tertiary ester moiety were synthesized and characterized. Polymer films containing a photoacid generator became insoluble in organic solvents on UV irradiation. The insoluble fraction of the irradiated films was increased by post-exposure-baking at relatively low temperatures (40-100 degreesC). When the cross-linked polymer films were baked at 120-200 degreesC, they became soluble in water. The effective bake temperature was dependent on the polymer structure. Thermal degradation of the cross-linked polymers was studied by TGA analysis and in situ FT-IR spectroscopy.
引用
收藏
页码:4075 / 4081
页数:7
相关论文
共 24 条
[1]  
Buchwalter SL, 1996, J POLYM SCI POL CHEM, V34, P249, DOI 10.1002/(SICI)1099-0518(19960130)34:2<249::AID-POLA11>3.0.CO
[2]  
2-Q
[3]   Characterization of thermally reworkable thermosets: materials for environmentally friendly processing and reuse [J].
Chen, JS ;
Ober, CK ;
Poliks, MD .
POLYMER, 2002, 43 (01) :131-139
[4]  
GRITSAI NI, 1967, J ORG CHEM USSR, V3, P1544
[5]  
Hitomi M, 1999, MACROMOL CHEM PHYSIC, V200, P1268, DOI 10.1002/(SICI)1521-3935(19990601)200:6<1268::AID-MACP1268>3.0.CO
[6]  
2-N
[7]  
Hitomi M, 1998, J POLYM SCI POL CHEM, V36, P2823, DOI 10.1002/(SICI)1099-0518(19981115)36:15<2823::AID-POLA19>3.0.CO
[8]  
2-H
[9]   Computational study of thermally controlled polymer network disassembly via the incorporation of sterically hindered urea linkages [J].
Malik, J ;
Clarson, SJ .
POLYMER, 2002, 43 (08) :2561-2567
[10]   The thermally controlled molecular disassembly properties of a polymer network via the incorporation of one sterically hindered urea linkage [J].
Malik, J ;
Clarson, SJ .
POLYMER DEGRADATION AND STABILITY, 2002, 76 (02) :241-249