Charged and Discharged States of Cathode/Sulfide Electrolyte Interfaces in All-Solid-State Lithium Ion Batteries

被引:80
作者
Sumita, Masato [1 ]
Tanaka, Yoshinori [2 ]
Ikeda, Minoru [1 ]
Ohno, Takahisa [1 ,2 ,3 ]
机构
[1] Natl Inst Mat Sci, 1-1 Namiki, Tsukuba, Ibaraki 3050044, Japan
[2] NIMS, Global Res Ctr Environm & Energy Based Nanomat, 1-1 Namiki, Tsukuba, Ibaraki 3050044, Japan
[3] Univ Tokyo, Inst Ind Sci, Meguro Ku, Tokyo 1538505, Japan
关键词
GLASS-CERAMIC ELECTROLYTES; SECONDARY BATTERIES; CRYSTAL-STRUCTURE; THIN-FILMS; CONDUCTOR; LI3PS4; CATHODE; LIFEPO4; SYSTEM; PHASE;
D O I
10.1021/acs.jpcc.6b01207
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
Interfaces between cathodes and sulfide electrolytes exhibit high resistance in all-solid-state lithium ion batteries. In this paper, to elucidate the origin of the high interface resistance we have theoretically investigated the properties of the cathode interfaces with the sulfide electrolyte and oxide electrolyte for comparison. From the density functional molecular dynamics simulations of the LiFePO4/Li3PS4 interface in both discharged and charged states, we have demonstrated the instability of the sulfide interface in the charged state, that is, the lithium depletion and oxidation on the sulfide side near the interface, in contrast to the oxide interfaces. The obtained results imply the formation of a Li-depleted layer around the sulfide interfaces during charging and support the validity of the insertion of oxide buffer layers at the interface to reduce the interface resistance.
引用
收藏
页码:13332 / 13339
页数:8
相关论文
共 33 条
[1]   Canonical sampling through velocity rescaling [J].
Bussi, Giovanni ;
Donadio, Davide ;
Parrinello, Michele .
JOURNAL OF CHEMICAL PHYSICS, 2007, 126 (01)
[2]   Recent developments in cathode materials for lithium ion batteries [J].
Fergus, Jeffrey W. .
JOURNAL OF POWER SOURCES, 2010, 195 (04) :939-954
[3]   Structural Evolution and Li Dynamics in Nanophase Li3PS4 by Solid-State and Pulsed-Field Gradient NMR [J].
Gobet, Mallory ;
Greenbaum, Steve ;
Sahu, Gayatri ;
Liang, Chengdu .
CHEMISTRY OF MATERIALS, 2014, 26 (11) :3558-3564
[4]   Separable dual-space Gaussian pseudopotentials [J].
Goedecker, S ;
Teter, M ;
Hutter, J .
PHYSICAL REVIEW B, 1996, 54 (03) :1703-1710
[5]   All-solid-state lithium batteries with Li3PS4 glass as active material [J].
Hakari, Takashi ;
Nagao, Motohiro ;
Hayashi, Akitoshi ;
Tatsumisago, Masahiro .
JOURNAL OF POWER SOURCES, 2015, 293 :721-725
[6]   Negligible "Negative Space-Charge Layer Effects" at Oxide-Electrolyte/Electrode Interfaces of Thin-Film Batteries [J].
Haruta, Masakazu ;
Shiraki, Susumu ;
Suzuki, Tohru ;
Kumatani, Akichika ;
Ohsawa, Takeo ;
Takagi, Yoshitaka ;
Shimizu, Ryota ;
Hitosugi, Taro .
NANO LETTERS, 2015, 15 (03) :1498-1502
[7]   Space-Charge Layer Effect at Interface between Oxide Cathode and Sulfide Electrolyte in All-Solid-State Lithium-Ion Battery [J].
Haruyama, Jun ;
Sodeyama, Keitaro ;
Han, Liyuan ;
Takada, Kazunori ;
Tateyama, Yoshitaka .
CHEMISTRY OF MATERIALS, 2014, 26 (14) :4248-4255
[8]   Invited Paper: Recent Development of Bulk-Type Solid-State Rechargeable Lithium Batteries with Sulfide Glass-ceramic Electrolytes [J].
Hayashi, Akitoshi ;
Tatsumisago, Masahiro .
ELECTRONIC MATERIALS LETTERS, 2012, 8 (02) :199-207
[9]   Development of sulfide glass-ceramic electrolytes for all-solid-state lithium rechargeable batteries [J].
Hayashi, Akitoshi ;
Minami, Keiichi ;
Tatsumisago, Masahiro .
JOURNAL OF SOLID STATE ELECTROCHEMISTRY, 2010, 14 (10) :1761-1767
[10]   Crystal Structure of High-Temperature Phase of Lithium Ionic Conductor, Li3PS4 [J].
Homma, Kenji ;
Yonemura, Masao ;
Nagao, Miki ;
Hirayama, Masaaki ;
Kanno, Ryoji .
JOURNAL OF THE PHYSICAL SOCIETY OF JAPAN, 2010, 79