摘要
Laboratory and industrial results are used to elucidate the general features of the deactivation of supported copper metal catalysts in hydrogenation reactions. Hydrogenations with copper catalysts are milder than with their nickel or platinum counterparts, and they have selectivities that are exploited commercially. They are used in single stream plants for production of hydrogen via the low-temperature water shift gas reaction, and for methanol manufacture from synthesis gas, and also in hydrogenation of speciality organic compounds. Common catalyst types are based on Cu/Cr2O3 (copper chromite) or Cu/ZnO formulations that contain stabilisers and promoters such as alkaline earth oxides and Al2O3. These have several roles, including inhibition of sintering, and poison traps that prevent poisoning of the active metal surface. The best understood are Cu/ZnO formulations that have improved sulphur resistance due to formation of thermodynamically stable ZnS. Copper catalysts are susceptible to thermal sintering via a surface migration process and this is markedly accelerated by the presence of even traces of chloride. Care must be, therefore, taken to eliminate halides from copper catalysts during manufacture, and from the reactants during use. Operating temperatures must be restricted, usually to below 300 degreesC when catalyst longevity is important with large catalyst volumes. Water can soften some Cu/ZnO formulations during use, and cause particle breakage that leads to high-pressure drop and maldistribution of flow through large catalyst beds and impaired performance. Commercial copper catalysts are not acidic, and since they operate under mild conditions, carbon deposition (coking) is uncommon. However, conventional site blocking poisoning with sulphur compounds, and particularly by H2S, is common. The initial phase involves interaction with surface hydroxyl groups and elimination of water. Sulphur is retained strongly on the catalyst, and when partially sulphided they can exhibit selectivity in hydrogenation of organic hydrogenations. A variety of other sulphur compounds, and some chlorinated organic compounds, can cause complete deactivation or enhanced selectivity. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:161 / 174
页数:14
相关论文
共 56 条
[1]  
Adkins H., 1931, J AM CHEM SOC, V53, P1091, DOI [10.1021/ja01354a041, DOI 10.1021/JA01354A041]
[2]   THEORY AND PRACTICE OF THE FORMULATION OF HETEROGENEOUS CATALYSTS [J].
ANDREW, SPS .
CHEMICAL ENGINEERING SCIENCE, 1981, 36 (09) :1431-1445
[3]  
ANDREW SPS, 1980, P 7 INT POST C S CAT
[4]  
ANDREW SPS, 1970, CATALYST HDB, P20
[5]   Effects of thiophene on CO adsorption and crotonaldehyde hydrogenation over silica-supported Pd-Cu catalysts [J].
Ashour, SS ;
Bailie, JE ;
Rochester, CH ;
Thomson, J ;
Hutchings, GJ .
JOURNAL OF MOLECULAR CATALYSIS A-CHEMICAL, 1997, 123 (01) :65-74
[6]   XPS STUDY ON BARIUM-PROMOTED COPPER CHROMITE CATALYSTS [J].
BIANCHI, CL ;
CATTANIA, MG ;
RAGAINI, V .
SURFACE AND INTERFACE ANALYSIS, 1992, 19 (1-12) :533-536
[7]  
BILVEN P, 1980, J CATAL, V63, P112
[8]  
BORTS MS, 1986, ZH PRIKL KHIM, V59, P126
[9]   THE HYDROGENATION OF FURFURALDEHYDE TO FURFURYL ALCOHOL AND SYLVAN (2-METHYLFURAN) [J].
BREMNER, JGM ;
KEEYS, RKF .
JOURNAL OF THE CHEMICAL SOCIETY, 1947, (AUG) :1068-1080
[10]   INFLUENCES OF CATALYST FORMULATION AND POISONING ON ACTIVITY AND DIE-OFF OF LOW TEMPERATURE SHIFT CATALYSTS [J].
CAMPBELL, JS .
INDUSTRIAL & ENGINEERING CHEMISTRY PROCESS DESIGN AND DEVELOPMENT, 1970, 9 (04) :588-&