Surface fluorination and electrochemical behavior of petroleum cokes graphitized at medium and high temperatures for secondary lithium battery

被引:29
作者
Li, JL
Naga, K
Ohzawa, Y
Nakajima, T [1 ]
Iwata, H
机构
[1] Aichi Inst Technol, Dept Appl Chem, Toyota 4700392, Japan
[2] Aichi Inst Technol, Tech Res Ctr, Toyota 4700392, Japan
关键词
surface modification; fluorination; carbon electrode; secondary lithium battery;
D O I
10.1016/j.jfluchem.2005.03.016
中图分类号
O61 [无机化学];
学科分类号
070301 ; 081704 ;
摘要
The surface structure and electrochemical performance have been investigated of petroleum cokes heat-treated at 2100 and 2600 degrees C (abbreviated to PC2100 and PC2600) and those fluorinated by elemental fluorine at 200 and 300 degrees C. XPS study indicated that surface fluorine was covalently bonded to carbon and surface fluorine contents were in the range of 4.9-17.8 at.%. Surface oxygen was reduced by fluorination. BET surface areas were nearly the same before and after fluorination. Fluorination enhanced D-band intensity in two Raman shifts observed at 15 80 cm(-1) (G-band) and 1360 cm(-1) (D-band), indicating the increase in the surface disordering. At a high current density of 150 mA/g, the capacity increase was observed for PC2100 fluorinated at 200 degrees C and for PC2600 fluorinated at 200 and 300 degrees C. The most interesting result was the increase in first coulombic efficiencies by surface fluorination. First columbic efficiencies for PC2600 fluorinated at 300 degrees C were increased by 12.1% at 60 mA/g and by 25.8% at 150 mA/g, respectively. The impedance measurements showed that the resistances of surface films on carbon electrodes were increased by fluorination, however, the charge transfer resistances were decreased by 12.3% for PC2100 fluorinated at 200 degrees C, and by 27.5 and 6.4% for PC2600 fluorinated at 200 and 300 degrees C, respectively. The reduction of the charge transfer resistances was consistent with increase in the charge capacities for PC2100 fluorinated at 200 degrees C and PC2600 fluorinated at 200 and 300 degrees C. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:1028 / 1035
页数:8
相关论文
共 22 条
[1]   Comparison between the electrochemical behavior of disordered carbons and graphite electrodes in connection with their structure [J].
Gnanaraj, JS ;
Levi, MD ;
Levi, E ;
Salitra, G ;
Aurbach, D ;
Fischer, JE ;
Claye, A .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 2001, 148 (06) :A525-A536
[2]   Electrochemical characteristics and structures of surface-fluorinated graphites with different particle sizes for lithium ion secondary batteries [J].
Gupta, V ;
Nakajima, T ;
Ohzawa, Y ;
Iwata, H .
JOURNAL OF FLUORINE CHEMISTRY, 2001, 112 (02) :233-240
[3]   Improvement on the electrochemical characteristics of graphite anodes by coating of the pyrolytic carbon using tumbling chemical vapor deposition [J].
Han, YS ;
Lee, JY .
ELECTROCHIMICA ACTA, 2003, 48 (08) :1073-1079
[4]  
Hara M., 1994, TANSO, V165, P261
[5]   CHARACTERIZATION OF DIAMOND FILMS BY RAMAN-SPECTROSCOPY [J].
KNIGHT, DS ;
WHITE, WB .
JOURNAL OF MATERIALS RESEARCH, 1989, 4 (02) :385-393
[6]   Nano-tube-like surface structure in graphite particles and its formation mechanism: A role in anodes of lithium-ion secondary batteries [J].
Moriguchi, K ;
Munetoh, S ;
Abe, M ;
Yonemura, M ;
Kamei, K ;
Shintani, A ;
Maehara, Y ;
Omaru, A ;
Nagamine, M .
JOURNAL OF APPLIED PHYSICS, 2000, 88 (11) :6369-6377
[7]  
Nakajima T, 2005, FLUORINATED MATERIALS FOR ENERGY CONVERSION, P1
[8]   Electrochemical behavior of surface-fluorinated graphite [J].
Nakajima, T ;
Koh, M ;
Singh, RN ;
Shimada, M .
ELECTROCHIMICA ACTA, 1999, 44 (17) :2879-2888
[9]   Electrochemical behavior of plasma-fluorinated graphite for lithium ion batteries [J].
Nakajima, T ;
Gupta, V ;
Ohzawa, Y ;
Koh, M ;
Singh, RN ;
Tressaud, A ;
Durand, E .
JOURNAL OF POWER SOURCES, 2002, 104 (01) :108-114
[10]   Surface structure and electrochemical properties of surface-fluorinated petroleum cokes for lithium ion battery [J].
Nakajima, T ;
Li, JL ;
Naga, K ;
Yoneshima, K ;
Nakai, T ;
Ohzawa, Y .
JOURNAL OF POWER SOURCES, 2004, 133 (02) :243-251