Degradation of bulk heterojunction solar cells operated in an inert gas atmosphere: a systematic study

被引:62
作者
Padinger, F [1 ]
Fromherz, T
Denk, P
Brabec, CJ
Zettner, J
Hierl, T
Sariciftci, NS
机构
[1] Quantum Solar Energy, Linz, Austria
[2] Johannes Kepler Univ, Linz Inst Organ Solar Cells, A-4040 Linz, Austria
[3] Thermosensor GmbH, Erlangen, Germany
关键词
organic solar cells; PPV and derivatives; fullerenes and derivatives; degradation; thermosensorical defect localization;
D O I
10.1016/S0379-6779(00)01504-6
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
We present a systematic study on the degradation of polymer/fullerene bulk heterojunction solar cells. Degradation behavior of photovoltaic devices based on poly [2-methoxy, 5-(3 ' ,7 ' -dimethyl-octyloxy)]-p-phenylene vinylene (MDMO-PPV) mixed with the soluble methanofullerene derivative [6,6]-Phenyl C-61-butyric acid methyl ester (PCBM) were investigated under inert gas atmosphere in the dark at room temperature, under enhanced temperature and under enhanced temperature together with illumination by white light at 80 mW/cm(2) light intensity. The influence on the degradation for exchanging the top electrode (Au instead of Al) was also investigated. Photothermal defect localization was performed on sealed polymer/fullerene photovoltaic devices.
引用
收藏
页码:1605 / 1606
页数:2
相关论文
共 2 条
[1]  
SHAHEEN SE, UNPUB APPL PHYS LETT
[2]   POLYMER PHOTOVOLTAIC CELLS - ENHANCED EFFICIENCIES VIA A NETWORK OF INTERNAL DONOR-ACCEPTOR HETEROJUNCTIONS [J].
YU, G ;
GAO, J ;
HUMMELEN, JC ;
WUDL, F ;
HEEGER, AJ .
SCIENCE, 1995, 270 (5243) :1789-1791