The evaporation time and wetting limit temperature for a water droplet on the surface of a bare, Zeolite-A-coated, or ZSM-5-coated stainless steel substrate have been experimentally studied. Three stainless steel substrates are prepared with different finishes. The surface finishing of a substrate is shown to cause observable changes in the wettability of a bare or ZSM-5-coated surface. Contact angle measurements reveal that Zeolite-A coatings are the most hydrophilic and that bare stainless steel is the least hydrophilic. The evaporation time and wetting limit temperature of a water droplet placed on the surface of the bare and coated substrates are examined as surface temperature increases. The zeolite coatings decrease the evaporation time and increase the wetting limit temperature on the bare stainless steel substrate, with Zeolite-A coatings offering the best improvement. For the bare substrate and the substrates coated with the same zeolite, as hydrophilicity increases, the evaporation time decreases and wetting limit temperature increases.
引用
收藏
页码:4310 / 4315
页数:6
相关论文
共 12 条
[1]   Corrosion-resistant zeolite coatings by in situ crystallization [J].
Cheng, XL ;
Wang, ZB ;
Yan, YS .
ELECTROCHEMICAL AND SOLID STATE LETTERS, 2001, 4 (05) :B23-B26
[2]   Hydrophilic surface formation on polymers by ion-assisted reaction [J].
Cho, JS ;
Kim, KH ;
Han, S ;
Beag, YW ;
Koh, SK .
PROGRESS IN ORGANIC COATINGS, 2003, 48 (2-4) :251-258
[3]   Performance of dehumidifying heat exchangers with and without wetting coatings [J].
Hong, K ;
Webb, RL .
JOURNAL OF HEAT TRANSFER-TRANSACTIONS OF THE ASME, 1999, 121 (04) :1018-1026
[4]   EFFECTS OF OXIDATION AND SURFACE-ROUGHNESS ON CONTACT-ANGLE [J].
HONG, KT ;
IMADOJEMU, H ;
WEBB, RL .
EXPERIMENTAL THERMAL AND FLUID SCIENCE, 1994, 8 (04) :279-285
[5]   Corrosion of central heating systems [J].
Jones, DRH .
ENGINEERING FAILURE ANALYSIS, 1997, 4 (03) :179-194
[6]   Plasma hydrophilic surface treatment for dehumidifying heat exchangers [J].
Kim, G ;
Lee, H ;
Webb, RL .
EXPERIMENTAL THERMAL AND FLUID SCIENCE, 2002, 27 (01) :1-10
[7]   Effects of hydrophilic surface treatment on evaporation heat transfer at the outside wall of horizontal tubes [J].
Kim, HY ;
Kang, BH .
APPLIED THERMAL ENGINEERING, 2003, 23 (04) :449-458
[8]  
Kwangtaek H, 2000, HVAC&R RES, V6, P229
[9]   Hydrophilic and antimicrobial zeolite coatings for gravity-independent water separation [J].
McDonnell, AMP ;
Beving, D ;
Wang, AJ ;
Chen, W ;
Yan, YS .
ADVANCED FUNCTIONAL MATERIALS, 2005, 15 (02) :336-340
[10]   PVD coatings as an environmentally clean alternative to electroplating and electroless processes [J].
Navinsek, B ;
Panjan, P ;
Milosev, I .
SURFACE & COATINGS TECHNOLOGY, 1999, 116 :476-487