Plasma wall interaction and its implication in an all tungsten divertor tokamak

被引:110
作者
Neu, R. [1 ]
Balden, M. [1 ]
Bobkov, V. [1 ]
Dux, R. [1 ]
Gruber, O. [1 ]
Herrmann, A. [1 ]
Kallenbach, A. [1 ]
Kaufmann, M. [1 ]
Maggi, C. F. [1 ]
Maier, H. [1 ]
Mueller, H. W. [1 ]
Puetterich, T. [1 ]
Pugno, R. [1 ]
Rohde, V. [1 ]
Sips, A. C. C. [1 ]
Stober, J. [1 ]
Suttrop, W. [1 ]
Angioni, C. [1 ]
Atanasiu, C. V. [1 ]
Becker, W. [1 ]
Behler, K. [1 ]
Behringer, K. [1 ]
Bergmann, A. [1 ]
Bertoncelli, T. [1 ]
Bilato, R. [1 ]
Bottino, A. [1 ]
Brambilla, M. [1 ]
Braun, F. [1 ]
Buhler, A. [1 ]
Chankin, A. [1 ]
Conway, G. [1 ]
Coster, D. P. [1 ]
de Marne, P. [1 ]
Dietrich, S. [1 ]
Dimova, K. [1 ]
Drube, R.
Eich, T.
Engelhardt, K. [1 ]
Fahrbach, H-U [1 ]
Fantz, U. [1 ]
Fattorini, L. [1 ,2 ]
Fink, J. [1 ]
Fischer, R. [1 ]
Flaws, A. [1 ]
Franzen, P. [1 ]
Fuchs, J. C. [1 ]
Gal, K. [1 ,3 ]
Garcia-Munoz, M. [1 ]
Gemisic-Adamov, M. [1 ]
Giannone, L. [1 ]
机构
[1] Max Planck Inst Plasma Phys, EURATOM Assoc, D-85748 Garching, Germany
[2] EURATOM Assoc IST, CFN, Lisbon, Portugal
[3] EURATOM Assoc HAS, KFKI, Budapest, Hungary
[4] EURATOM Assoc Tekes, HUT, Helsinki, Finland
[5] EURATOM Assoc ENEA, Consorzio RFX, Padua, Italy
[6] CRPP EPFL, CH-1051 Lausanne, Switzerland
[7] Univ Coll Cork, Phys Dept, Assoc EURATOM DCU, Cork, Ireland
[8] EURATOM Assoc RISO, NL Riso, Roskilde, Denmark
[9] Stuttgart Germany, Inst Plasmaforsch, Stuttgart, Germany
[10] Univ Innsbruck, EURATOM Assoc OAW, A-6020 Innsbruck, Austria
关键词
D O I
10.1088/0741-3335/49/12B/S04
中图分类号
O35 [流体力学]; O53 [等离子体物理学];
学科分类号
070204 ; 080103 ; 080704 ;
摘要
ASDEX Upgrade has recently finished its transition towards an all-W divertor tokamak, by the exchange of the last remaining graphite tiles to W-coated ones. The plasma start-up was performed without prior boronization. It was found that the large He content in the plasma, resulting from DC glow discharges for conditioning, leads to a confinement reduction. After the change to D glow for inter-shot conditioning, the He content quickly dropped and, in parallel, the usual H-Mode confinement with H factors close to one was achieved. After the initial conditioning phase, oxygen concentrations similar to that in previous campaigns with boronizations could be achieved. Despite the removal of all macroscopic carbon sources, no strong change in C influxes and C content could be observed so far. The W concentrations are similar to the ones measured previously in discharges with old boronization and only partial coverage of the surfaces with W. Concomitantly it is found that although the W erosion flux in the divertor is larger than the W sources in the main chamber in most of the scenarios, it plays only a minor role for the W content in the main plasma. For large antenna distances and strong gas puffing, ICRH power coupling could be optimized to reduce the W influxes. This allowed a similar increase of stored energy as yielded with comparable beam power. However, a strong increase of radiated power and a loss of H-Mode was observed for conditions with high temperature edge plasma close to the antennas. The use of ECRH allowed keeping the central peaking of the W concentration low and even phases of improved H-modes have already been achieved.
引用
收藏
页码:B59 / B70
页数:12
相关论文
共 29 条
  • [1] The ITER design
    Aymar, R
    Barabaschi, P
    Shimomura, Y
    [J]. PLASMA PHYSICS AND CONTROLLED FUSION, 2002, 44 (05) : 519 - 565
  • [2] Plasma facing and high heat flux materials - needs for ITER and beyond
    Bolt, H
    Barabash, V
    Federici, G
    Linke, J
    Loarte, A
    Roth, J
    Sato, K
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2002, 307 : 43 - 52
  • [3] Particle exhaust studies in ASDEX Upgrade
    Bosch, HS
    Coster, D
    Dux, R
    Haas, G
    Kallenbach, A
    Kaufmann, M
    Lackner, K
    Neuhauser, J
    Hempel, SD
    Poschenrieder, W
    Schneider, R
    [J]. PLASMA PHYSICS AND CONTROLLED FUSION, 1997, 39 (11) : 1771 - 1792
  • [4] Tungsten erosion at the ICRH limiters in ASDEX upgrade
    Dux, R.
    Bobkov, V.
    Fedorczak, N.
    Iraschko, K.
    Kallenbach, A.
    Neu, R.
    Puetterich, T.
    Rohde, V.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2007, 363 : 112 - 116
  • [5] Influence of the heating profile on impurity transport in ASDEX Upgrade
    Dux, R
    Neu, R
    Peeters, AG
    Pereverzev, G
    Mück, A
    Ryter, F
    Stober, J
    [J]. PLASMA PHYSICS AND CONTROLLED FUSION, 2003, 45 (09) : 1815 - 1825
  • [6] DUX R, 2007, P 34 EPS C PLASM PHY, P1
  • [7] Determination of the tungsten divertor retention at ASDEX Upgrade using a sublimation probe
    Geier, A
    Maier, H
    Neu, R
    Krieger, K
    [J]. PLASMA PHYSICS AND CONTROLLED FUSION, 2002, 44 (10) : 2091 - 2100
  • [8] The requirements of a next step large steady state tokamak
    Janeschitz, G
    Barabaschi, P
    Federici, G
    Ioki, K
    Ladd, P
    Mukhovatov, V
    Sugihara, M
    Tivey, R
    [J]. NUCLEAR FUSION, 2000, 40 (06) : 1197 - 1221
  • [9] Spectroscopic investigation of carbon migration with tungsten walls in ASDEX Upgrade
    Kallenbach, A.
    Dux, R.
    Harhausen, J.
    Maggi, C. F.
    Neu, R.
    Puetterich, T.
    Rohde, V.
    Schmid, K.
    Wolfrum, E.
    [J]. JOURNAL OF NUCLEAR MATERIALS, 2007, 363 : 60 - 65
  • [10] Tokamak operation with high-Z plasma facing components
    Kallenbach, A
    Neu, R
    Dux, R
    Fahrbach, HU
    Fuchs, JC
    Giannone, L
    Gruber, O
    Herrmann, A
    Lang, PT
    Lipschultz, B
    Maggi, CF
    Neuhauser, J
    Philipps, V
    Pütterich, T
    Rohde, V
    Roth, J
    Sergienko, G
    Sips, A
    [J]. PLASMA PHYSICS AND CONTROLLED FUSION, 2005, 47 : B207 - B222