Processing of carbon-fiber-reinforced Zr41.2Ti13.8Cu12.5Ni10.0Be22.5 bulk metallic glass composites

被引:110
作者
Kim, CP
Busch, R [1 ]
Masuhr, A
Choi-Yim, H
Johnson, WL
机构
[1] Oregon State Univ, Dept Mech Engn, Corvallis, OR 97331 USA
[2] CALTECH, WM Keck Lab Engn Mat, Pasadena, CA 91125 USA
关键词
D O I
10.1063/1.1390317
中图分类号
O59 [应用物理学];
学科分类号
摘要
Carbon-fiber-reinforced bulk metallic glass composites are produced by infiltrating liquid Zr41.2Ti13.8Cu12.5Ni10.0Be22.5 into carbon fiber bundles with diameter of the individual fiber of 5 mum. Reactive wetting occurs by the formation of a ZrC layer around the fibers. This results in a composite with a homogeneous fiber distribution. The volume fraction of the fibers is about 50% and the density of the composite amounts to 4.0 g/cm(3). (C) 2001 American Institute of Physics.
引用
收藏
页码:1456 / 1458
页数:3
相关论文
共 7 条
[1]   Synthesis and characterization of particulate reinforced Zr57Nb5Al10Cu15.4Ni12.6 bulk metallic glass composites [J].
Choi-Yim, H ;
Busch, R ;
Köster, U ;
Johnson, WL .
ACTA MATERIALIA, 1999, 47 (08) :2455-2462
[2]   Bulk metallic glass matrix composites [J].
Choi-Yim, H ;
Johnson, WL .
APPLIED PHYSICS LETTERS, 1997, 71 (26) :3808-3810
[3]   The effect of silicon on the glass forming ability of the Cu47Ti34Zr11Ni8 bulk metallic glass forming alloy during processing of composites [J].
Choi-Yim, H ;
Busch, R ;
Johnson, WL .
JOURNAL OF APPLIED PHYSICS, 1998, 83 (12) :7993-7997
[4]   Melt infiltration casting of bulk metallic-glass matrix composites [J].
Dandliker, RB ;
Conner, RD ;
Johnson, WL .
JOURNAL OF MATERIALS RESEARCH, 1998, 13 (10) :2896-2901
[5]   Mechanically alloyed Zr55Al10Cu30Ni5 metallic glass composites containing nanocrystalline W particles [J].
Eckert, J ;
Kübler, A ;
Schultz, L .
JOURNAL OF APPLIED PHYSICS, 1999, 85 (10) :7112-7119
[6]  
LIN XH, 1997, MATER T JIM, V38, P475
[7]   A HIGHLY PROCESSABLE METALLIC-GLASS - ZR41.2TI13.8CU12.5NI10.0BE22.5 [J].
PEKER, A ;
JOHNSON, WL .
APPLIED PHYSICS LETTERS, 1993, 63 (17) :2342-2344