Dichloropentafluoropropanes as solvents for size exclusion chromatography

被引:25
作者
Isemura, T
Kakita, R
Kawahara, K
机构
[1] Asahi Glass Co Ltd, Analyt Technol Grp, Qual Assurance Off, Chem Co, Ichihara, Chiba 2908566, Japan
[2] Asahi Glass Co Ltd, Res Ctr, Kanagawa Ku, Yokohama, Kanagawa 2218755, Japan
关键词
mobile phase composition; polymers; dichloropentafluoropropanes; poly(methyl methacrylate); polyamide; poly(ethylene terephthalate); hexafluoroisopropanol; poly(2-(perfluoroalkyl)ethyl acrylate); perfluoropolyether; nylon;
D O I
10.1016/j.chroma.2003.11.003
中图分类号
Q5 [生物化学];
学科分类号
071010 ; 081704 ;
摘要
We have found that HCFC225s (HCFC225ca: 3,3-dichloro-1, 1, 1,2,2-pentafluoropropane, HCFC225cb: 1,3-dichloro-1,1,2,2,3-pentafluoropropane) are superior mobile phases for size exclusion chromatography (SEC). As alternatives of CFC113, they have been shown to possess a number of excellent properties, such as low flammability, low viscosity, low cost, high purity, and environmental and operational friendliness. In addition, they have distinct advantages for the SEC measurement, because they solubilize some kinds of acrylate such as poly(methyl methacrylate) (PMMA) and commercial monodispersed PMMA can be used to prepare calibration curves necessary for the measurement of equivalent molecular weight of some polymers. Furthermore, we propose an HCFC225/1,1,1,3,3,3-hexafluoroisopropanol mixed solvent for use in the SEC of poly(ethylene terephthalate) (PET) and polyamides. Poly(2-(perfluorooctyl)ethyl acrylate), whose PMMA equivalent weight average molecular weight was 118, 100 Da, was evaluated by a multi-angle laser light scattering (MALLS) detector to have an absolute molecular weight of 439,000 Da: The difference can be attributed to the molecular size of the polyfluorinated polymer compared to the non-fluorinated one. The possible application of this novel mobile phase system for molecular size and molecular weight characterization of perfluoropolyethers, PET, nylon 6 and nylon 6,6 are also discussed. (C) 2003 Elsevier B.V. All rights reserved.
引用
收藏
页码:109 / 116
页数:8
相关论文
共 11 条
[1]  
GEMMEL B, 1995, CHEM FIBRES INT, V45, P104
[2]   MOLECULAR-WEIGHT CHARACTERIZATION OF FLUOROPOLYOXYALKYLENES BY GEL-PERMEATION CHROMATOGRAPHY [J].
GIANOTTI, G ;
LEVI, M ;
TURRI, S .
JOURNAL OF APPLIED POLYMER SCIENCE, 1994, 51 (06) :973-978
[3]   EFFECT OF HYDROGEN SUBSTITUTION ON THE MASS-SPECTROMETRY AND SIZE-EXCLUSION CHROMATOGRAPHY OF PERFLUORINATED POLYETHER FLUIDS AS DETERMINED BY TIME-OF-FLIGHT SECONDARY ION MASS-SPECTROMETRY [J].
HUES, SM ;
WYATT, JR ;
COLTON, RJ ;
BLACK, BH .
ANALYTICAL CHEMISTRY, 1990, 62 (10) :1074-1079
[4]   CYCLIC OLIGOMER CONSIDERATIONS IN THE SIZE-EXCLUSION CHROMATOGRAPHY OF POLY(ETHYLENE-TEREPHTHALATE) [J].
MARTIN, L ;
BALKE, ST .
JOURNAL OF LIQUID CHROMATOGRAPHY, 1995, 18 (01) :1-15
[6]   EFFECTS OF ADDITION OF AN ELECTROLYTE ON SIZE-EXCLUSION CHROMATOGRAPHY OF POLYAMIDES USING HEXAFLUORO-2-PROPANOL AS MOBILE-PHASE [J].
MORI, S ;
NISHIMURA, Y .
JOURNAL OF LIQUID CHROMATOGRAPHY, 1993, 16 (16) :3359-3370
[7]  
MORONI A, 1997, POLYM MAT SCI ENG, V77, P14
[8]   Size-exclusion chromatography in 1,1,1,3,3,3-hexafluoro-2-propanol [J].
Mourey, TH ;
Bryan, TG .
JOURNAL OF CHROMATOGRAPHY A, 2002, 964 (1-2) :169-178
[9]  
SAKAI M, 1983, BUNSEKI KAGAKU, V32, P258
[10]   INTRINSIC-VISCOSITY AND MOLECULAR-WEIGHT MEASUREMENT OF NYLON-66 POLYMERS [J].
SAMANTA, SR .
JOURNAL OF APPLIED POLYMER SCIENCE, 1992, 45 (09) :1635-1640