Nanostructured ceramic oxides with a slow crack growth resistance close to covalent materials

被引:62
作者
Chevalier, J
Deville, S
Fantozzi, G
Bartolomé, JF
Pecharroman, C
Moya, JS
Diaz, LA
Torrecillas, R
机构
[1] Inst Natl Sci Appl, CNRS, UMR 5510, Dept Mat, F-69621 Villeurbanne, France
[2] CSIC, Spanish Res Council, ICMM, Madrid, Spain
[3] CSIC, Spanish Res Council, INCAR, Oviedo 33080, Spain
关键词
D O I
10.1021/nl050492j
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
Oxide ceramics are sensitive to slow crack growth because adsorption of water can take place at the crack tip, leading to a strong decrease of the surface energy in humid (or air) conditions. This is a major drawback concerning demanding, long-term applications such as orthopaedic implants. Here we show that a specific nanostructuration of ceramic oxides can lead to a crack resistance never reached before, similar to that of covalent ceramics.
引用
收藏
页码:1297 / 1301
页数:5
相关论文
共 17 条
[1]   Influence of the metal particle size on the crack growth resistance in mullite-molybdenum composites [J].
Bartolomé, JF ;
Díaz, M ;
Moya, JS .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (11) :2778-2784
[2]  
Bartolome JF, 1998, J AM CERAM SOC, V81, P1502, DOI 10.1111/j.1151-2916.1998.tb02509.x
[3]  
Chevalier J, 2000, ADV MATER, V12, P1619, DOI 10.1002/1521-4095(200011)12:21<1619::AID-ADMA1619>3.0.CO
[4]  
2-O
[5]  
CHEVALIER J, 2001, CERAMICS BIOMEDICAL
[6]  
ELATTAOUI H, 2005, IN PRESS J AM CERAM
[7]   WHY CAN MICROCRACKS IN CERAMICS PROPAGATE AT EXTREMELY LOW STRESS INTENSITY FACTORS [J].
FETT, T ;
MUNZ, D .
JOURNAL OF MATERIALS SCIENCE LETTERS, 1992, 11 (05) :257-260
[8]   STABILITY OF TETRAGONAL ZRO2 PARTICLES IN CERAMIC MATRICES [J].
HEUER, AH ;
CLAUSSEN, N ;
KRIVEN, WM ;
RUHLE, M .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1982, 65 (12) :642-650
[9]   Crack stability and strength variability in alumina ceramics with rising toughness-curve behavior [J].
Kovar, D ;
Bennison, SJ ;
Readey, MJ .
ACTA MATERIALIA, 2000, 48 (02) :565-578
[10]   FATIGUE LIMITS IN NONCYCLIC LOADING OF CERAMICS WITH CRACK-RESISTANCE CURVES [J].
LATHABAI, S ;
LAWN, BR .
JOURNAL OF MATERIALS SCIENCE, 1989, 24 (12) :4298-4306