共 33 条
[1]
FACTORS AFFECTING INTERNAL-FRICTION PEAK DUE TO THERMOELASTIC MARTENSITIC-TRANSFORMATION
[J].
SCRIPTA METALLURGICA,
1976, 10 (12)
:1125-1128
[2]
DEJONGHE W, 1977, MET SCI NOV, P523
[3]
DEJONGHE W, 1975, SHAPE MEMORY EFFECTS, P451
[4]
DELORME JF, 1971, J PHYS, P101
[5]
EUCKEN S, 1990, MATER SCI FORUM, V56, P487
[6]
THE B2 TO R TRANSFORMATION IN TI50NI47FE3 AND TI49.5NI50.5 ALLOYS
[J].
ACTA METALLURGICA,
1985, 33 (09)
:1717-1723
[8]
THE INVESTIGATION OF INTERNAL-FRICTION, ELECTRIC-RESISTANCE AND SHAPE CHANGE IN NITI ALLOY DURING PHASE-TRANSFORMATIONS
[J].
SCRIPTA METALLURGICA,
1985, 19 (09)
:1033-1038
[9]
THE INFLUENCE OF STRESS ON THE INTERNAL-FRICTION, ELECTRIC-RESISTANCE, SHAPE CHANGE IN NITI ALLOY DURING PHASE-TRANSFORMATIONS
[J].
SCRIPTA METALLURGICA,
1985, 19 (09)
:1039-1044
[10]
TRANSFORMATION BEHAVIOR OF A TI50NI47FE3 ALLOY .2. SUBSEQUENT PREMARTENSITIC BEHAVIOR AND THE COMMENSURATE PHASE
[J].
PHILOSOPHICAL MAGAZINE A-PHYSICS OF CONDENSED MATTER STRUCTURE DEFECTS AND MECHANICAL PROPERTIES,
1983, 47 (01)
:31-62