Corrosion of mullite by molten salts

被引:40
作者
Jacobson, NS [1 ]
Lee, KN [1 ]
Yoshio, T [1 ]
机构
[1] OKAYAMA UNIV, OKAYAMA 700, JAPAN
关键词
D O I
10.1111/j.1151-2916.1996.tb08951.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The interaction of molten salts of different Na2O activities and mullite is examined with furnace and burner tests. The more-acidic molten salts form small amounts of Al2O3; the more-basic molten salts form various Na2O-Al2O3-SiO2 compounds. The results are interpreted using the Na2O-Al2O3-SiO2 ternary phase diagram, and some possible diffusion paths are discussed. The generally higher melting points of Na2O-Al2O3-SiO2 compounds lead to better behavior of mullite in molten salts, as compared to SiO2-protected ceramics such as SIC. Mullite-coated SIC is discussed, and the corrosion behavior is evaluated.
引用
收藏
页码:2161 / 2167
页数:7
相关论文
共 21 条
[1]  
[Anonymous], SUPERALLOYS 2
[2]  
[Anonymous], 1973, IRON STEEL ENG
[3]  
Barin I, 1989, THERMOCHEMICAL PROPE
[4]  
BROWN JJ, 1994, PHASE DIAGRAMS ADV C, P43
[5]   THE STABILITY OF BETA-AL2O3(NA2O.11AL2O3) IN OXYGEN ATMOSPHERES [J].
ELREFAIE, FA ;
SMELTZER, WW .
JOURNAL OF THE ELECTROCHEMICAL SOCIETY, 1981, 128 (07) :1443-1447
[6]   ALUMINA BASE COATINGS FOR PROTECTION OF SIC CERAMICS [J].
FEDERER, JI .
JOURNAL OF MATERIALS ENGINEERING, 1990, 12 (02) :141-149
[7]  
Gordon S, 1971, NASA SP-273, Technical Report
[8]   SODIUM-SULFATE - DEPOSITION AND DISSOLUTION OF SILICA [J].
JACOBSON, NS .
OXIDATION OF METALS, 1989, 31 (1-2) :91-103
[9]  
JACOBSON NS, 1992, HIGH TEMPERATURE COR, P514
[10]  
JACOBSON NS, 1986, ADV CERAM MATER, V1, P154