Molecular dynamics simulation of the structure and hydroxylation of silica glass surfaces

被引:154
作者
Du, JC [1 ]
Cormack, AN [1 ]
机构
[1] Alfred Univ, New York State Coll Ceram, Ctr Glass Res, Alfred, NY 14802 USA
关键词
D O I
10.1111/j.1551-2916.2005.00352.x
中图分类号
TQ174 [陶瓷工业]; TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The surface structure of silica glasses has been simulated using molecular dynamics. The surface hydroxyl concentration was estimated to be 4.5/nm(2), based on surface defect statistics. Hydroxyl-silica potentials were developed and used to study the hydroxylation of silica surface. It is found that the energy of chemisorption of water declines in the sequence: three coordinated silicon (Si-3) and non-bridging oxygen (NBO) on separate sites, Si-3 and NBO on combined sites, two- and three-membered rings. Partial hydroxylation of the most reactive sites, which leads to an OH coverage of 2.5/nm(2), was studied. Structural relaxation after hydroxylation was observed.
引用
收藏
页码:2532 / 2539
页数:8
相关论文
共 50 条
[1]   On the computer simulation of a hydrophobic vitreous silica surface [J].
Bakaev, VA ;
Steele, WA .
JOURNAL OF CHEMICAL PHYSICS, 1999, 111 (21) :9803-9812
[2]   Atomistic simulation of hydroxide ions in inorganic solids [J].
Baram, PS ;
Parker, SC .
PHILOSOPHICAL MAGAZINE B-PHYSICS OF CONDENSED MATTER STATISTICAL MECHANICS ELECTRONIC OPTICAL AND MAGNETIC PROPERTIES, 1996, 73 (01) :49-58
[3]   HYDROPHILIC AND HYDROPHOBIC SITES ON DEHYDRATED CRYSTALLINE AND AMORPHOUS SILICAS [J].
BOLIS, V ;
FUBINI, B ;
MARCHESE, L ;
MARTRA, G ;
COSTA, D .
JOURNAL OF THE CHEMICAL SOCIETY-FARADAY TRANSACTIONS, 1991, 87 (03) :497-505
[4]   KINETICS OF DISSOCIATIVE CHEMISORPTION ON STRAINED EDGE-SHARED SURFACE-DEFECTS ON DEHYDROXYLATED SILICA [J].
BUNKER, BC ;
HAALAND, DM ;
MICHALSKE, TA ;
SMITH, WL .
SURFACE SCIENCE, 1989, 222 (01) :95-118
[5]   MOLECULAR MECHANISMS FOR CORROSION OF SILICA AND SILICATE-GLASSES [J].
BUNKER, BC .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1994, 179 :300-308
[6]   INFRARED-SPECTRA OF EDGE-SHARED SILICATE TETRAHEDRA [J].
BUNKER, BC ;
HAALAND, DM ;
WARD, KJ ;
MICHALSKE, TA ;
SMITH, WL ;
BINKLEY, JS ;
MELIUS, CF ;
BALFE, CA .
SURFACE SCIENCE, 1989, 210 (03) :406-428
[7]   Porous silica-water interactions .1. Structural and dimensional changes induced by water adsorption [J].
Burneau, A ;
Lepage, J ;
Maurice, G .
JOURNAL OF NON-CRYSTALLINE SOLIDS, 1997, 217 (01) :1-10
[8]  
CORMACK AN, 1998, TOPICAL ISSUES GLASS, V2
[9]  
D'Souza AS, 1999, J AM CERAM SOC, V82, P1289, DOI 10.1111/j.1151-2916.1999.tb01909.x
[10]   Hydroxylation and dehydroxylation behavior of silica glass fracture surfaces [J].
D'Souza, AS ;
Pantano, CG .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 2002, 85 (06) :1499-1504