Experimental set-up for thermopower and resistivity measurements at 100-1300 K

被引:168
作者
Burkov, AT [1 ]
Heinrich, A
Konstantinov, PP
Nakama, T
Yagasaki, K
机构
[1] Russian Acad Sci, AF Ioffe Phys Tech Inst, St Petersburg 196140, Russia
[2] Univ Ryukyus, Fac Sci, Dept Phys, Okinawa 9030213, Japan
[3] Inst Solid State & Mat Res, Dresden, Germany
关键词
thermopower; electrical resistivity; high temperatures; thin films;
D O I
10.1088/0957-0233/12/3/304
中图分类号
T [工业技术];
学科分类号
08 ;
摘要
In this paper we describe an experimental set-up for simultaneous measurements of thermopower and electrical resistivity at temperatures from 100 K to 1300 K. Optimal configuration of electrodes and original mechanical contacts of thermocouples, current leads and potential probes with the sample make it possible to measure a large variety of materials and result in greater flexibility with respect to the sample form and dimensions. Both bulk and thin film samples with resistances in the range from 0 Omega up to 200 k Omega (1 G Omega in case of the resistivity measurement) can be investigated. Precision and high reliability of the system have been proven during more than three years of use. The resistivity and thermopower of pure Pb, Cu and Ni, and a Cr-Si thin film composite are presented as test materials to demonstrate the possibilities and accuracy of this experimental set-up.
引用
收藏
页码:264 / 272
页数:9
相关论文
共 15 条
[1]  
Barnard R. D., 1972, THERMOELECTRICITY ME
[2]  
BEYLIN VM, 1975, PHYS MET METALLOGR, V39, P63
[3]   MAGNON-DRAG THERMOPOWER IN IRON [J].
BLATT, FJ ;
FLOOD, DJ ;
ROWE, V ;
SCHROEDER, PA ;
COX, JE .
PHYSICAL REVIEW LETTERS, 1967, 18 (11) :395-+
[4]  
BORELIUS G, 1928, 196A COMM PHYS LAB
[5]   THE ABSOLUTE SCALE OF THERMOELECTRIC POWER AT HIGH TEMPERATURE [J].
CUSACK, N ;
KENDALL, P .
PROCEEDINGS OF THE PHYSICAL SOCIETY OF LONDON, 1958, 72 (467) :898-901
[6]   MEASUREMENTS OF THOMSON COEFFICIENTS FOR METALS AT HIGH TEMPERATURES AND OF PELTIER COEFFICIENTS FOR SOLID-LIQUID INTERFACES OF METALS [J].
LANDER, JJ .
PHYSICAL REVIEW, 1948, 74 (04) :479-488
[7]   TRANSPORT PROPERTIES OF FERROMAGNETIC METALS .2. NICKEL [J].
LAUBITZ, MJ ;
MATSUMURA, T ;
KELLY, PJ .
CANADIAN JOURNAL OF PHYSICS, 1976, 54 (01) :92-102
[8]   THERMAL DIFFUSIVITY OF PLATINUM FROM 300 DEGREES TO 1200 DEGREES K [J].
MARTIN, JJ ;
SIDLES, PH ;
DANIELSO.GC .
JOURNAL OF APPLIED PHYSICS, 1967, 38 (08) :3075-&
[9]   ABSOLUTE SEEBECK COEFFICIENT OF PLATINUM FROM 80 TO 340 K AND THERMAL AND ELECTRICAL CONDUCTIVITIES OF LEAD FROM 80 TO 400 K [J].
MOORE, JP ;
GRAVES, RS .
JOURNAL OF APPLIED PHYSICS, 1973, 44 (03) :1174-1178
[10]  
NEMCHENKO VF, 1970, PHYS METALS METALLOG, V30, P202