Thermal degradation of polyethylene mixed with poly(vinyl chloride) and poly(ethyleneterephthalate)

被引:83
作者
Sakata, Y [1 ]
Uddin, MA [1 ]
Koizumi, K [1 ]
Murata, K [1 ]
机构
[1] MITSUI ENGN & SHIP BLDG CO LTD,CHIBA 290,JAPAN
关键词
D O I
10.1016/0141-3910(96)00077-8
中图分类号
O63 [高分子化学(高聚物)];
学科分类号
070305 ; 080501 ; 081704 ;
摘要
Thermal degradation of plastics such as polyethylene (PE), poly(vinylchloride) (PVC), poly(ethyleneterephthalate) (PET) and their mixtures (PE + PVC and PE + PET) was studied at 430 degrees C by batch operation to analyse the conversion of waste plastics into fuel oil. A visual inspection of the inside of the reactor was made and the macroscopic process of degradation was monitored. Products of degradation were classified into three groups: gases, liquids and residues in the reactor. The degradation of PE produced liquid products which consisted of C-5-C-25 fraction of hydrocarbons with a yield of 70 wt%. On the other hand, the degradation of PVC produced only 4.7 wt% liquid products which consisted of C-5-C-20 fraction of hydrocarbons and the degradation of PET produced no liquid products. The effect of mixing PVC and PET with PE on the yield and compositions of liquid products was investigated. The addition of either PVC or PET to PE decreased the overall liquid products yield; however, it promoted the degradation of PE into low molecular weight liquid hydrocarbon products. (C) 1996 Published by Elsevier Science Limited.
引用
收藏
页码:111 / 117
页数:7
相关论文
共 12 条
  • [1] THERMAL-DECOMPOSITION OF POLYSTYRENE - EFFECT OF MOLECULAR-WEIGHT
    FUNT, JM
    MAGILL, JH
    [J]. JOURNAL OF POLYMER SCIENCE PART B-POLYMER PHYSICS, 1974, 12 (01) : 217 - 220
  • [2] KAMINSKY W, 1993, PRECISION PROCESS TECHNOLOGY, P65
  • [3] PREPARATION OF ACTIVATED CARBON FROM SCRAPPED POLYVINYL-CHLORIDE)
    KASAOKA, S
    SAKATA, Y
    YAMATO, H
    NISHIYAMA, T
    [J]. NIPPON KAGAKU KAISHI, 1980, (06) : 858 - 864
  • [4] KASAOKA S, 1980, INT CHEM ENG, V20, P446
  • [5] THERMOLYSIS OF POLYETHYLENE
    MCCAFFREY, WC
    KAMAL, MR
    COOPER, DG
    [J]. POLYMER DEGRADATION AND STABILITY, 1995, 47 (01) : 133 - 139
  • [6] PRIMARY THERMAL-DEGRADATION MECHANISMS OF PET AND PBT
    MONTAUDO, G
    PUGLISI, C
    SAMPERI, F
    [J]. POLYMER DEGRADATION AND STABILITY, 1993, 42 (01) : 13 - 28
  • [7] THERMAL-DEGRADATION OF POLYSTYRENE
    MURATA, K
    MAKINO, T
    [J]. NIPPON KAGAKU KAISHI, 1975, (07) : 1241 - 1248
  • [8] THERMAL-DEGRADATION OF MIXED POLYMER
    MURATA, K
    AKIMOTO, M
    [J]. NIPPON KAGAKU KAISHI, 1979, (06) : 774 - 781
  • [9] THERMAL-DEGRADATION OF POLYPROPYLENE
    MURATA, K
    MAKINO, T
    [J]. NIPPON KAGAKU KAISHI, 1975, (01) : 192 - 200
  • [10] MURATA K, 1973, NIPPON KAGAKUKAISHI, P2214