The effects of silicone fluid additives and silicone elastomer matrices on barnacle adhesion strength

被引:74
作者
Kavanagh, CJ
Swain, GW
Kovach, BS
Stein, J
Darkangelo-Wood, C
Truby, K
Holm, E
Montemarano, J
Meyer, A
Wiebe, D
机构
[1] Florida Inst Technol, Dept Oceanog & Ocean Engn, Melbourne, FL 32901 USA
[2] GE Global Res Ctr, Niskayuna, NY 12309 USA
[3] NSWCCD, Bethesda, MD 20084 USA
[4] SUNY Buffalo, Buffalo, NY 14214 USA
[5] Altran Corp, Boston, MA 02210 USA
关键词
PDMS elastomeric coatings; silicone fluid additives; fouling-release; ASTM D-5618; adhesion strength; Balanus eburneus;
D O I
10.1080/08927010310001623296
中图分类号
Q81 [生物工程学(生物技术)]; Q93 [微生物学];
学科分类号
071005 ; 0836 ; 090102 ; 100705 ;
摘要
Barnacle adhesion strength was used to screen seventy-seven polydimethylsiloxane elastomeric coatings for fouling-release properties. The test coatings were designed to investigate the effect on barnacle adhesion strength of silicone fluid additive type, additive location, additive molecular weight, additive loading level, mixtures of additives, coating matrix type and coating fillers. The type of silicone fluid additive was the primary controlling factor in barnacle fouling-release. The type of silicone matrix in which the fluid resided was found to alter the effect on fouling-release. Two PDMS fluids, DMSC15 and DBE224, significantly reduced the adhesion strength of barnacles compared to unmodified elastomers. Optimum fouling-release performance was dependent on the interaction of fluid type and elastomeric matrix.
引用
收藏
页码:381 / 390
页数:10
相关论文
共 25 条
[1]  
[Anonymous], 1987, SILICON COMPOUNDS RE
[2]  
ARKLES B, 1995, SILICON GERMANIUM TI, P432
[3]   ADHESION - MECHANISMS THAT ASSIST OR IMPEDE IT [J].
BAIER, RE ;
SHAFRIN, EG ;
ZISMAN, WA .
SCIENCE, 1968, 162 (3860) :1360-&
[4]  
Brady RF, 2000, J COATING TECHNOL, V72, P44
[5]   Mechanical factors favoring release from fouling release coatings [J].
Brady, RF ;
Singer, IL .
BIOFOULING, 2000, 15 (1-3) :73-81
[6]  
Callow M. E., 1988, Biodeterioration 7. Selected papers presented at the 7th International Biodeterioration Symposium, Cambridge, UK, September 1987., P43
[7]  
Callow ME., 1986, STUDIES ENV SCI, P145
[8]   RESISTANCE TO MARINE FOULING OF ELASTOMERIC COATINGS OF SOME POLY(DIMETHYLSILOXANES) AND POLY(DIMETHYLDIPHENYLSILOXANES) [J].
EDWARDS, DP ;
NEVELL, TG ;
PLUNKETT, BA ;
OCHILTREE, BC .
INTERNATIONAL BIODETERIORATION & BIODEGRADATION, 1994, 34 (3-4) :349-359
[9]  
FINZEL WA, 1996, FEDERATION SERIES CO, P1