Preparation of (La1-xSrx)MnO3 by coprecipitation method
被引:12
作者:
Uehara, M
Takahashi, K
Asaka, T
Tsutsumi, S
机构:
[1] Natl Inst Res Inorgan Mat, Tsukuba, Ibaraki 3050044, Japan
[2] Waseda Univ, Sch Educ, Inst Earth Sci, Shinjuku Ku, Tokyo 1698050, Japan
关键词:
coprecipitation method;
perovskite;
CMR;
(La;
Sr)MnO3;
homogeneity;
compositional fluctuation;
D O I:
10.2109/jcersj.106.1248
中图分类号:
TQ174 [陶瓷工业];
TB3 [工程材料学];
学科分类号:
0805 ;
080502 ;
摘要:
ii coprecipitate of the carbonate was first obtained by the titration of sodium carbonate into solution in which MnO, SrCO3, and La2O3 were dissolved by hydrochloric acid, Heating the coprecipitate for Ih at 600 degrees C, 7 h at 1000 degrees C, and successively 10 h at 1300 degrees C produced a sintered body of (La1-xSrx) MnO3, which was observed by electron microscopy and analyzed by X-ray powder diffratometory, As a result, it was clarified that the coprecipitation method enables to obtain the single phase in the range of x=0.4-0.6, which is not possible by the dry process. Even in the range x=0.2-0.4, where both the methods enable to obtain the single phase, the samples prepared by the coprecipitation method had better homogeneity and smaller compositional fluctuation than these prepared dry method.