Evolution of optimal porosity for improved hydrogen storage in templated zeolite-like carbons

被引:60
作者
Alam, Nurul [1 ]
Mokaya, Robert [1 ]
机构
[1] Univ Nottingham, Sch Chem, Nottingham NG7 2RD, England
关键词
METAL-ORGANIC FRAMEWORKS; HIGH-SURFACE-AREA; ORDERED POROUS CARBON; CHEMICAL-VAPOR-DEPOSITION; CARBIDE-DERIVED CARBONS; MICROPOROUS CARBONS; ACTIVATED CARBONS; PORE-SIZE; STRUCTURAL REGULARITY; MESOPOROUS CARBONS;
D O I
10.1039/c0ee00154f
中图分类号
O6 [化学];
学科分类号
0703 ;
摘要
The microporosity of zeolite-like carbons, prepared using zeolite Y as hard template via a two-step carbon ingress route involving liquid impregnation with furfuryl alcohol followed by chemical vapour deposition (CVD) of acetonitrile, can be varied by changing the CVD temperature. Carbons prepared at CVD temperature of 700 to 900 degrees C have surface area of ca. 2000 m(2) g(-1), pore volume of ca. 1 cm(3) g(-1) and micropore size distribution in the 6-25 angstrom range. The proportion of microporosity in the templated carbons is very high at between 87 and 91% of surface area, while 73 to 83% of pore volume is associated with micropores. The XRD patterns and TEM images of carbons prepared at CVD temperatures of 700, 750 and 800 degrees C confirm the presence of zeolite-like pore channel ordering and the absence of graphitisation. More importantly, the pore size of the carbons can be varied by changing the CVD temperature so as to optimise the formation of ultramicropores of size 6 angstrom. Templated carbons that possess a significant proportion of ultramicropores exhibit unexpectedly higher hydrogen uptake than that of samples with higher total and micropore surface area but with fewer ultramicropores. The interaction between carbon and hydrogen in the ultramicropore containing carbons is stronger with isosteric heat of adsorption of 9.5 kJ mol(-1) compared to 6 kJ mol(-1) for samples with fewer or no ultramicropores. This stronger interaction leads to higher specific hydrogen uptake of up to 14 mu mol H(2) m(-2), one of the highest ever observed for high surface area microporous carbon.
引用
收藏
页码:1773 / 1781
页数:9
相关论文
共 87 条
[1]   Vehicular storage of hydrogen in insulated pressure vessels [J].
Aceves, Salvador M. ;
Berry, Gene D. ;
Martinez-Frias, Joel ;
Espinosa-Loza, Francisco .
INTERNATIONAL JOURNAL OF HYDROGEN ENERGY, 2006, 31 (15) :2274-2283
[2]   NMR Methods for Characterizing the Pore Structures and Hydrogen Storage Properties of Microporous Carbons [J].
Anderson, Robert J. ;
McNicholas, Thomas P. ;
Kleinhammes, Alfred ;
Wang, Anmiao ;
Liu, Jie ;
Wu, Yue .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 2010, 132 (25) :8618-8626
[3]   Role of microporosity in hydrogen adsorption on templated nanoporous carbons [J].
Armandi, M. ;
Bonelli, B. ;
Arean, C. Otero ;
Garrone, E. .
MICROPOROUS AND MESOPOROUS MATERIALS, 2008, 112 (1-3) :411-418
[4]   Pore structure of carbon-mineral nanocomposites and derived carbons obtained by template carbonization [J].
Bandosz, TJ ;
Jagiello, J ;
Putyera, K ;
Schwarz, JA .
CHEMISTRY OF MATERIALS, 1996, 8 (08) :2023-2029
[5]   Structured carbon adsorbents from clay, zeolite and mesoporous aluminosilicate templates [J].
Barata-Rodrigues, PM ;
Mays, TJ ;
Moggridge, GD .
CARBON, 2003, 41 (12) :2231-2246
[6]   Optimum conditions for adsorptive storage [J].
Bhatia, SK ;
Myers, AL .
LANGMUIR, 2006, 22 (04) :1688-1700
[7]   Adsorption of gases in multimolecular layers [J].
Brunauer, S ;
Emmett, PH ;
Teller, E .
JOURNAL OF THE AMERICAN CHEMICAL SOCIETY, 1938, 60 :309-319
[8]   Hydrogen storage capacities of nanoporous carbon calculated by density functional and Moller-Plesset methods [J].
Cabria, I. ;
Lopez, M. J. ;
Alonso, J. A. .
PHYSICAL REVIEW B, 2008, 78 (07)
[9]   The optimum average nanopore size for hydrogen storage in carbon nanoporous materials [J].
Cabria, Ivan ;
Lopez, Maria J. ;
Alonso, Julio A. .
CARBON, 2007, 45 (13) :2649-2658
[10]   Biomass waste-derived microporous carbons with controlled texture and enhanced hydrogen uptake [J].
Cheng, Fangyi ;
Liang, Jing ;
Zhao, Jianzhi ;
Tao, Zhanliang ;
Chen, Jun .
CHEMISTRY OF MATERIALS, 2008, 20 (05) :1889-1895