Catalytic degradation of plastic waste to liquid fuel over commercial cracking catalysts - Effect of polymer to catalyst ratio/acidity content

被引:116
作者
Akpanudoh, NS [1 ]
Gobin, K [1 ]
Manos, G [1 ]
机构
[1] UCL, Dept Chem Engn, London WC1E 7JE, England
基金
英国工程与自然科学研究理事会;
关键词
polymer degradation; catalytic cracking; fuel; polymer recycling;
D O I
10.1016/j.molcata.2005.03.009
中图分类号
O64 [物理化学(理论化学)、化学物理学];
学科分类号
070304 ; 081704 ;
摘要
The catalytic degradation of polyethylene over two commercial cracking catalysts, containing 20% and 40% ultrastable Y zeolite, respectively, was studied in a semi-batch reactor. More specifically, the effect of the polymer to catalyst ratio - expressed as the acidity content of the polymer/catalyst system - was studied on the formation of liquid hydrocarbons. After a sharp increase at small values, the liquid yield seemed to have a negative correlation to the acidity content, showing a maximum at acidity values around 7% of pure US-Y. Regarding the boiling point distribution of the liquid fraction in systems with higher content of active catalyst, a shift was generally observed towards lighter products. Comparing liquid samples during the same experiment, later samples contained heavier components with the exception of the system with the smallest US-Y content of this study. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:67 / 73
页数:7
相关论文
共 18 条
[1]   Transformation of several plastic wastes into fuels by catalytic cracking [J].
Arandes, JM ;
Abajo, I ;
LopezValerio, D ;
Fernandez, I ;
Azkoiti, MJ ;
Olazar, M ;
Bilbao, J .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1997, 36 (11) :4523-4529
[2]   Valorization by thermal cracking over silica of polyolefins dissolved in LCO [J].
Arandes, JM ;
Ereña, J ;
Azkoiti, MJ ;
López-Valerio, D ;
Bilbao, J .
FUEL PROCESSING TECHNOLOGY, 2004, 85 (2-3) :125-140
[3]  
Arguado J., 1997, ENERG FUEL, V11, P1225
[4]   CATALYTIC DEGRADATION OF POLYOLEFINS [J].
AUDISIO, G ;
BERTINI, F ;
BELTRAME, PL ;
CARNITI, P .
MAKROMOLEKULARE CHEMIE-MACROMOLECULAR SYMPOSIA, 1992, 57 :191-209
[5]   Coke formation during catalytic cracking of C8 aliphatic hydrocarbons over ultrastable Y zeolite [J].
Brillis, AA ;
Manos, G .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2003, 42 (11) :2292-2298
[6]   Recycled plastics in FCC feedstocks: Specific contributions [J].
delaPuente, G ;
Arandes, JM ;
Sedran, UA .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 1997, 36 (11) :4530-4534
[7]   Polymer degradation to fuels over microporous catalysts as a novel tertiary plastic recycling method [J].
Gobin, K ;
Manos, G .
POLYMER DEGRADATION AND STABILITY, 2004, 83 (02) :267-279
[8]   Catalytic degradation of high-density polyethylene on an ultrastable-Y zeolite. Nature of initial polymer reactions, pattern of formation of gas and liquid products, and temperature effects [J].
Manos, G ;
Garforth, A ;
Dwyer, J .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2000, 39 (05) :1203-1208
[9]   Catalytic degradation of high-density polyethylene over different zeolitic structures [J].
Manos, G ;
Garforth, A ;
Dwyer, J .
INDUSTRIAL & ENGINEERING CHEMISTRY RESEARCH, 2000, 39 (05) :1198-1202
[10]   Tertiary recycling of polyethylene to hydrocarbon fuel by catalytic cracking over aluminum pillared clays [J].
Manos, G ;
Yusof, IY ;
Gangas, NH ;
Papayannakos, N .
ENERGY & FUELS, 2002, 16 (02) :485-489