Reaction of sodium calcium borate glasses to form hydroxyapatite

被引:64
作者
Han, Xue
Day, Delbert E.
机构
[1] Johns Hopkins Univ, Dept Mat Sci & Engn, Baltimore, MD 21218 USA
[2] Univ Missouri, Grad Ctr Mat Res, Rolla, MO 65409 USA
[3] Univ Missouri, Dept Ceram Engn, Rolla, MO 65409 USA
关键词
D O I
10.1007/s10856-007-3053-2
中图分类号
R318 [生物医学工程];
学科分类号
0831 ;
摘要
This study investigated the transformation of two sodium calcium borate glasses to hydroxyapatite ( HA). The chemical reaction was between either 1CaO center dot 2Na(2)O center dot 6B(2)O(3) or 2CaO center dot 2Na(2)O center dot 6B(2)O(3) glass and a 0.25 M phosphate (K2HPO4) solution at 37, 75 and 200 degrees C. Glass samples in the form of irregular particles (125-180 mu m) and microspheres (45-90 and 125-180 mu m) were used in order to understand the reaction mechanism. The effect of glass composition ( calcium content) on the weight loss rate and reaction temperature on crystal size, crystallinity and grain shape of the reaction products were studied. Carbonated HA was made by dissolving an appropriate amount of carbonate (K2CO3) in the 0.25 M phosphate solution. X-ray diffraction, Fourier transform infrared spectroscopy, and scanning electron microscopy were used to characterize the reaction products. The results show that sodium calcium borate glasses can be transformed to HA by reacting with a phosphate solution. It is essentially a process of dissolution of glass and precipitation of HA. The transformation begins from an amorphous state to calcium-deficient HA without changing the size and shape of the original glass sample. Glass with a lower calcium content ( 1CaO center dot 2Na(2)O center dot 6B(2)O(3)), or reacted at an elevated temperature ( 75 degrees C), has a higher reaction rate. The HA crystal size increases and grain shape changes from spheroidal to cylindrical as temperature increases from 37 to 200 degrees C. Increase in carbonate concentration can also decrease the crystal size and yield a more needle-like grain shape.
引用
收藏
页码:1837 / 1847
页数:11
相关论文
共 23 条
[1]  
BARBA II, 2000, J BIOMED MATER RES, V51, P191
[2]  
Barralet J, 1998, J BIOMED MATER RES, V41, P79, DOI 10.1002/(SICI)1097-4636(199807)41:1<79::AID-JBM10>3.0.CO
[3]  
2-C
[4]   In vitro behavior of albumin-loaded carbonate hydroxyapatite gel [J].
Barralet, JE ;
Aldred, S ;
Wright, AJ ;
Coombes, AGA .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 2002, 60 (03) :360-367
[5]   An analysis of hydroxyapatite surface layer formation [J].
Brown, PW ;
Martin, RI .
JOURNAL OF PHYSICAL CHEMISTRY B, 1999, 103 (10) :1671-1675
[6]   FTIR study of adsorption of CO2 on nonstoichiometric calcium hydroxyapatite [J].
Cheng, ZH ;
Yasukawa, A ;
Kandori, K ;
Ishikawa, T .
LANGMUIR, 1998, 14 (23) :6681-6686
[7]  
Clark DE., 1979, CORROSION OF GLASS
[8]   In vitro and in vivo dissolution behavior of a dysprosium lithium borate glass designed for the radiation synovectomy treatment of rheumatoid arthritis [J].
Conzone, SD ;
Brown, RF ;
Day, DE ;
Ehrhardt, GJ .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 2002, 60 (02) :260-268
[9]   Biomimetic apatite through a self-assembly process [J].
Du, C ;
Cui, FZ ;
de Groot, K ;
Layrolle, P .
BIOCERAMICS 14, 2002, 218-2 :39-42
[10]   Novel synthesis and characterization of an AB-type carbonate-substituted hydroxyapatite [J].
Gibson, IR ;
Bonfield, W .
JOURNAL OF BIOMEDICAL MATERIALS RESEARCH, 2002, 59 (04) :697-708