SiC fiber strength after consolidation and heat-treatment in Ti-22Al-23Nb matrix composite

被引:12
作者
Gambone, ML
机构
[1] Wright Laboratory, Materials Directorate, Wright-Patterson AFB, OH
关键词
D O I
10.1016/S0956-716X(95)00546-8
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
[No abstract available]
引用
收藏
页码:507 / 512
页数:6
相关论文
共 14 条
[1]  
BANERJEE D, 1993, STRUCTURAL INTERMETALLICS, P19
[2]  
GAMBONE ML, 1994, INTERMETALLICS COMPO, V350, P111
[3]   THE EVALUATION OF THE STRENGTH DISTRIBUTION OF SILICON-CARBIDE AND ALUMINA FIBERS BY A MULTIMODAL WEIBULL DISTRIBUTION [J].
GODA, K ;
FUKUNAGA, H .
JOURNAL OF MATERIALS SCIENCE, 1986, 21 (12) :4475-4480
[4]  
JAKUS K, 1981, J AM CERAM SOC, V64, pC174, DOI 10.1111/j.1151-2916.1981.tb15904.x
[5]  
Johnson L, 1964, STATISTICAL TREATMEN, P37
[6]   THE MICROSTRUCTURE OF SCS-6 SIC FIBER [J].
NING, XJ ;
PIROUZ, P .
JOURNAL OF MATERIALS RESEARCH, 1991, 6 (10) :2234-2248
[7]   SILICON-CARBIDE FILAMENTS - MICROSTRUCTURE [J].
NUTT, SR ;
WAWNER, FE .
JOURNAL OF MATERIALS SCIENCE, 1985, 20 (06) :1953-1960
[8]  
OCHIAI S, 1979, J MATER SCI, V14, P831
[9]  
ROWE RG, 1991, SYNTHESIS PROCESSING
[10]  
Smith P. R., 1992, WLTR924035, P115