Thick ceramic thermal barrier coatings with high durability deposited using solution-precursor plasma spray

被引:97
作者
Jadhav, A
Padture, NP [1 ]
Wu, F
Jordan, EH
Gell, M
机构
[1] Univ Connecticut, Inst Mat Sci, Dept Mat Sci & Engn, Storrs, CT 06269 USA
[2] Univ Connecticut, Inst Mat Sci, Dept Mech Engn, Storrs, CT 06269 USA
来源
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING | 2005年 / 405卷 / 1-2期
关键词
thermal barrier coatings; plasma spray; toughness; compression; thermal cycling;
D O I
10.1016/j.msea.2005.06.023
中图分类号
TB3 [工程材料学];
学科分类号
0805 ; 080502 ;
摘要
The efficacy of ceramic thermal barrier coatings (TBCs) used to protect and insulate metal components in engines increases with the thickness of the TBCs. However, the durabilities of thick TBCs deposited using conventional ceramics-coating deposition methods have not been adequate. Here, we demonstrate the feasibility of depositing highly durable, 4 mm thick TBCs of ZrO2-7 wt.% Y2O3 (7YSZ) on bond-coated superalloy substrates using the solution-precursor plasma spray (SPPS) method. It was found that the average thermal cycling life of the 4 mm thick SPPS TBCs is 820 cycles. While most of the conventional air plasma-sprayed (APS) coatings of the same composition and thickness deposited on identical bond-coated superalloy substrates were found to be detached partially from the substrates in the as-sprayed condition, the APS TBC that was intact failed after 40 thermal cycles. The dramatic improvement in the thermal cycling life in the SPPS TBCs can be attributed to: (i) the significantly higher in-plane indentation-fracture toughness (over five-fold) in the SPPS TBCs over APS TBCs and (ii) the presence of the vertical cracks in SPPS TBCs resulting in a high degree of strain tolerance. The large thickness of the SPPS coatings also allowed us to characterize the mechanical properties of the ceramic top-coat in some detail. To that end, we report here the results from indentation-toughness tests and uniaxial-compression tests on the SPPS TBCs and the reference APS TBCs. (c) 2005 Elsevier B.V. All rights reserved.
引用
收藏
页码:313 / 320
页数:8
相关论文
共 32 条
[1]  
[Anonymous], [No title captured]
[2]  
[Anonymous], 1996, Metallurgical and Ceramic Protective Coatings
[3]  
[Anonymous], THERMAL CONDUCTIVITY
[4]  
[Anonymous], SCI ENG THERMAL SPRA
[5]   FAILURE MECHANISMS OF A ZIRCONIA-8 WT-PERCENT YTTRIA THERMAL BARRIER COATING [J].
BARTLETT, AH ;
DALMASCHIO, R .
JOURNAL OF THE AMERICAN CERAMIC SOCIETY, 1995, 78 (04) :1018-1024
[6]  
BEARDSLEY MB, 1990, P 1990 COAT ADV HEAT, P1153
[7]   Mechanisms of ceramic coating deposition in solution-precursor plasma spray [J].
Bhatia, T ;
Ozturk, A ;
Xie, LD ;
Jordan, EH ;
Cetegen, BM ;
Gell, M ;
Ma, XQ ;
Padture, NP .
JOURNAL OF MATERIALS RESEARCH, 2002, 17 (09) :2363-2372
[8]  
Choi SR, 2004, INT J APPL CERAM TEC, V1, P330
[9]   Mechanisms controlling the durability of thermal barrier coatings [J].
Evans, AG ;
Mumm, DR ;
Hutchinson, JW ;
Meier, GH ;
Pettit, FS .
PROGRESS IN MATERIALS SCIENCE, 2001, 46 (05) :505-553
[10]   Mechanisms of spallation of solution precursor plasma spray thermal barrier coatings [J].
Gell, M ;
Xie, LD ;
Jordan, EH ;
Padture, NP .
SURFACE & COATINGS TECHNOLOGY, 2004, 188 :101-106