A comparison of slurry erosion characteristics of TiNi shape memory alloys and SUS304 stainless steel

被引:50
作者
Lin, HC
Wu, SK [1 ]
Yeh, CH
机构
[1] Natl Taiwan Univ, Dept Mech Engn, Taipei 106, Taiwan
[2] Feng Chia Univ, Dept Mat Sci, Taichung 407, Taiwan
[3] Natl Taiwan Univ, Inst Mat Sci & Engn, Taipei 106, Taiwan
基金
日本学术振兴会;
关键词
liquid/solid impingement erosion; TiNi alloys; SUS304 stainless steel; thermoelastic martensitic transformation;
D O I
10.1016/S0043-1648(01)00580-4
中图分类号
TH [机械、仪表工业];
学科分类号
0802 ;
摘要
The slurry erosion characteristics of three TiNi shape memory alloys and SUS304 stainless steel using the liquid/solid impingement have been systematically studied. Experimental results show that more resistant TiNi alloys and less resistant SUS304 stainless steel exhibit ductile behavior and the maximum erosion has observed at 30 degrees. The surface morphologies exhibit many long furrows and ridges at low impingement angles. The exponent in the relation epsilon = kV(n) varied between 2 and 3 for impingement angles between 15 degrees and 90 degrees. Work hardening of surface is observed on the surface of all tested materials. The work hardening layer and thin platelet formation increase with angle of impingement. The SIM formation and pseudoelastic behavior of TiNi B2 phase, and variant accommodation and SIP formation of TiNi martensite, make important contributions to the slurry erosion resistance of TiNi alloys. (C) 2001 Elsevier Science B.V. All rights reserved.
引用
收藏
页码:557 / 565
页数:9
相关论文
共 36 条
[1]   THE ABRASIVE-CORROSIVE WEAR OF STAINLESS-STEELS [J].
ALLEN, C ;
BALL, A ;
PROTHEROE, BE .
WEAR, 1981, 74 (02) :287-305
[2]  
APTEKAR SS, 1985, WEAR MAT 1985, P677
[3]  
*ASTM, 1995, G7695 ASTM
[4]  
*ASTM, 1993, G7393 ASTM
[5]   ON THE IMPORTANCE OF WORK-HARDENING IN THE DESIGN OF WEAR-RESISTANT MATERIALS [J].
BALL, A .
WEAR, 1983, 91 (02) :201-207
[6]   EROSION MECHANISM IN DUCTILE METALS [J].
BELLMAN, R ;
LEVY, A .
WEAR, 1981, 70 (01) :1-27
[7]  
Castleman L.S., 1981, BIOCOMPATIBILITY CLI, V1, P129
[8]   TRIBOLOGICAL BEHAVIOR OF A TITANIUM NICKEL-ALLOY [J].
CLAYTON, P .
WEAR, 1993, 162 :202-210
[9]   RESISTANCE OF PURE METALS TO LOW STRESS ABRASIVE WEAR - COMMENTS [J].
DEGEE, AWJ .
WEAR, 1982, 81 (02) :373-374
[10]   VELOCITY DEPENDENCE OF EROSION OF DUCTILE METALS BY SOLID PARTICLES AT LOW ANGLES OF INCIDENCE [J].
FINNIE, I ;
MCFADDEN, DH .
WEAR, 1978, 48 (01) :181-190